HomeLearning CenterRTV cylinder mold cutting of Akron rtv-rp
  • Description

    Mold cutting Akron RTV-RP clear silicone. Cylinder mold was cured in a round film canister which saves about 1/2 the normal amount of silicone. RP master was designed by Diannah Beauregard in western North Carolina. RP master was built at Rio Grande with DM220 resin.

  • Author

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.