Keum-Boo
- Length57 minutes 48 seconds
- Description
Master goldsmith Charles Lewton-Brain lectures about and demonstrates how to make Keum-Boo foil and use the technique. This a method of applying thin sheets of pure gold to silver and other metals. This gives great design and pattern options and raises the value of a silver object at a low cost. Filmed in full HD 1080p.
- Includes
Purchase also includes these instructional PDF downloads:
- KeumBooLewtonBrain17.pdf
- KeumBooNotes.pdf
- AuthorCharles Lewton-Brain
Master goldsmith Charles Lewton-Brain trained, studied and worked in Germany, Canada and the United States to learn the skills he uses. Charles Lewton-Brain is one of the original creators of Ganoksin.
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.