Wax Casting Burnout Cycles
If you are experiencing rough surfaces, discolored metal or no-fills, the problem may be in the burnout. When casting, the...
Read More
The Sprue System Design
A very high percentage of investment casting defects can be directly or indirectly attributed to the design of the sprue...
Read More
950 Palladium: Custom Made Components
When making custom jewelry with any alloy, certain components within the piece are often hand made to enhance the final...
Read More
Sand Casting Method
Though sand casting has been largely replaced by centrifugal casting in recent decades, for hundreds of years it was the...
Read More
Cuttlefish Casting Method
Cuttlefish casting is a quick and fairly accurate casting method. Its applications are limited only by the thickness and overall...
Read More
Important Principles of Casting Safety
Here's something to aim for: a well laid-out, orderly workshop, well-lit by multiple non glare light sources, well-maintained equipment, electrically...
Read More
Natural Rubber or Silicone Rubber?
Natural rubber or silicone rubber? In the world of lost wax casting, this question is hardly an academic one. The...
Read More
Casting Notes for Silver Lost Wax Casting
Casting of silver can be fairly easy and these notes are the results of my experience through trial and error...
Read More
Sand Casting Safety Notes
Sand casting is used extensively for large-scale casting, such as engine blocks, and the grates that one sees around trees...
Read More
Casting Investment Powder Performances
In each step of manufacturing jewelry, there are many factors that can adversely affect quality. Because of this, process control...
Read More
Identifying and Preventing Wax Defects
Manufacturer spend much time and money diagnosing defects that are believed to originate in the casting process, but actually occur...
Read More
950 Palladium Bench Guide
The palladium bench guide reviews the working characteristics of palladium for the jewelry bench staff and provides an overview of...
Read More
Platinum Durability vs Scratching
There is a major difference between durability and scratch resistance. Platinum is very durable. When scratched, the scratch actually displaces...
Read More
Casting Investment Materials and Applications
The casting investment process enjoys wide popularity in the production of commercial and one-of-a-kind art metal objects. However, production practice...
Read More
Understanding the Process of Platinum Casting
Platinum casting is different from gold or silver casting, and insufficient preparation and understanding of the process can still lead...
Read More
Cracks in Jewelry Manufacturing
As many jewelry manufacturers and goldsmiths know from hard experience, cracking in jewelry can occur at any time during its...
Read More
Platinum Jewelry Advanced Joining Techniques
Joining is a very important production technique in the field of jewelry production. Therefore it is useful to know, what...
Read More
Damascus and Pattern Welding
True damascus steel is made by a casting process utilizing very high carbon steel. The material is held at or...
Read More
Five Steps for Successful Investing
A good practice for preventing investment blowout is to measure the height of the trees before investing. The maximum tree...
Read More
Bi-Metal Casting to Titanium
Titanium and the other refractory metals other the metalsmith a new range of exotic colors - colors that are beautiful...
Read More
Creating a Rubber Mold
Recently this
custom ring design
came to my bench
with the request that
it be made in platinum and a...
Read More
Using dental mold-making materials in jewelry making
Jewelers are always molding objects and parts, most often to use for making wax models for casting. There are many...
Read More
Investment Procedure for Lost Wax Casting
Clean, fresh investment, water and investment at room temperature, de-ionized or distilled water or water that has been sitting overnight....
Read More
De-oxidized Sterling Silver Alloys
Sterling silver alloys typically contain about 7.5 percent copper, an addition that not only provides strength to the otherwise pure...
Read More
Identification & Correction of Platinum Casting Defects
Platinum casting defects are often very difficult to characterize due to the intrinsic complexity of the investment casting process. All...
Read More
Casting an Orchid Flower
Everybody scampers for executing orders in a rush against all odds to satisfy customers or - if you'#39;re lucky -...
Read More
Causes & Prevention of Defects in Wrought Alloys
Much of the recent literature on defects that occur in jewellery manufacture is focused on those occurring in lost wax...
Read More
Making Silver Wire
Making silver wire
Read More
Setting Stones in Wax
One of the most revolutionary advances in recent years, apart from laser welding, is the method of setting stones in...
Read More
How to Make a Wax Injector
You will require a 5 to 6 inch by 3 inch wide brass or copper tube, silver solder a cover...
Read More
950 Palladium: White Metal Alloys
Of late, an increasing number of white precious metal alloys have been introduced into the jewelry marketplace in answer to...
Read More
Alloying Gold for Granulation
An alloy is by definition a mixture of two or more metals to create different strengths and colors. For granulation,...
Read More
Alloys – Look on the White Side
In the jewelry industry, it's rare to have an alloy without drawbacks, particularly when the alloy is not yellow. When...
Read More
The Art of Mold Cutting
Mold cutting sounds simple enough: Using a sharp knife and a simple tool, such as a can opener or a...
Read More
Frequently Used Wax Tools
Dental probes and knives make good wax tools. Your local dentist or dental hygienist or school for the same can...
Read More
Platinum Casting Investments
In this paper I will attempt to give some insight into the investments used to cast Platinum and also talk...
Read More
5 Classic Casting Tips
These slow, quiet days of summer are always a good time to review your shop practices before the busy holiday...
Read More
Preparing 3D Acrylic Photopolymer Patterns
Editors Note: This article is excerpted from “A New Method for Preparing 3D Acrylic Photopolymer Patterns for Investment Casting,” a...
Read More
Cutting a Rubber Mold
In my first article I made a rubber "sandwich" mold of this basket style mounting. The focus of this article...
Read More
Tips for Casting Palladium
Some manufacturers jumped at the chance to work with palladium a few years ago, when it made its way into...
Read More
Molding Alternatives for Jewelers
Jewelers need to make molds of objects and parts frequently. Usually wax is poured into the molds and the results...
Read More
Wax Model Carving
Recently a customer requested that we make her an unusual mother's ring. She chose a magnificent 3.56 ct. oval blue...
Read More
Using Dental Mold-Making Materials
Jewelers are always molding objects and parts, most often to use for making wax models for casting. There are many...
Read More
An Overview of Platinum Casting
As in all manufacturing processes, evaluations and systematic process controls must be applied to platinum casting. As a caster you...
Read More
Retracing Steps to Solve Casting Problems
A design riddled with undercuts and sharp little details just screams casting nightmare the moment the CAD file shows up....
Read More
950 Palladium: Setting Fabrication
This simple pendant design will be made with 950 palladium wire. Tack-welding technology will be used to temporarily hold the...
Read More
What Causes Casting Marks?
In the Spring 2003 Issue we asked the question "What causes these marks on this casting?" Around 100 readers responded...
Read More
Testing the New HD Patterns
Invented by Victor Joyner, a Chicagobased manufacturing jeweler, patented High Definition (HD) Patterns are made of a light-curing polymer material...
Read More
Creating a Two Tone Ring
In this issue I'm going to walk you through the creation of a ring with two different colors of gold....
Read More
Cast Hinges for Jewelers and Goldsmiths
Cast hinges are a very important part of much production jewelry work, partly because hinge assembly on such pieces is...
Read More
950 Palladium: Selling Points
Designers and manufacturers have embraced 950 palladium alloys for a variety of jewelry manufacturing products. At the recent JA Jewelry...
Read More
Casting Tools and Products
This segment from the 2017 MJSA Journal November issue is dedicated to metals, tools, software and more that aids jewelers...
Read More
Exhibition of Contemporary Japanese Metalwork
Quoting the scholar, Nyozekan Hasegawa, Masataka Ogawa Calls Japan the country of "the culture of hands." Over the centuries, no...
Read More
Precious Metal Clay 101
There are two brands of metal clay available today; Precious Metal Clay and Art Clay Silver. There are a lot...
Read More
950 Palladium: Manufacturing Tips and Techniques
The "other white metal" is making its presence known and it wont be long before light, bright and white 950...
Read More
Firescale Prevention During Vacuum Casting
Firescale has been the scourge of sterling silver casters since the first silver was poured into a mold. It has...
Read More
Eliminating Ash Residue Defects
The casting department at Stuller Inc. in Lafayette, Louisiana, has been experimenting with casting photopolymer models, and it has found...
Read More
John Killmaster and “The Quickening”
In the early 1980's, I made a drawing based on the theme of transformation, a sudden, intuitive grasp of reality...
Read More
Lost Wax Casting Part 3 of 9 Steam Dewaxing
This video was originally created to explain the casting process we use at Feathered Gems to the client whose charms...
Read More
Platinum Casting with Gemstones
Platinum casting with gemstones in place has been the latest development before the end of the second millennium. It has...
Read More
Testing the Ultra-Vest MAXX Investment
AJM recently asked Linus Drogs of AU Enterprises in Berkley , Michigan , to test the new Ultra-Vest MAXX Investment...
Read More
950 Palladium: Laser Welding Techniques
According to Frank McAllister, the quantity of individual pieces of jewelry made from 950 palladium has surpassed the same for...
Read More
Simple Platinum Casting
Filmed at Kraftwerks from PM West, Robert Lumabao demonstrates a unique system of flask-less platinum casting. Narrator Daniel Ballard, takes...
Read More
Overcoming Lightweight Casting Challenges
It's no wonder that as precious metals prices have risen to new heights over the past few years, jewelry castings...
Read More
Platinum Casting Process Control
It is widely known that platinum, the most noble of metals, is also the most challenging of metals. Platinum's high...
Read More
Etype Automated Wax Injection System
Racine and his son, Ittai, a physicist by profession but a top engineer, passed on purchasing the dated facility and...
Read More
950 Palladium: Manufacturing Methods
Palladium, long used as a luxurious jewelry metal, has recently experienced renewed interest largely due to its purity, natural white...
Read More
Carving Your Wax Piece with Kate Wolf
Creative Side Jewelry Academy of Austin presents Kate Wolf, owner of Wolf Tools, as she uses the Wolf Trimmer to...
Read More
Gold Casting Machine,gold making machinery,Jewellery casting
Gold Casting Machine,gold making machinery,Jewellery casting Equipment,Jewellery Casting Machine,Jewellery Casting Process,Jewellery Casting Technique,jewellery making machinery,silver Casting Machine,silver casting techniqe,Auto Pouring...
Read More
Tip for Improving Casting Quality
Every caster has seen his or her fair share of investment inclusions. You'll be polishing a casting when suddenly a...
Read More
Casting Gold to Platinum for the Jewelry Industry
The principle of bi-metal casting is really very simple: A wax model is invested, cast and finished. A secondary wax...
Read More
950 Palladium: Successful Design Considerations
Well designed 950 palladium jewelry plays to the strengths of this unique metal -- the aesthetics of its light, bright,...
Read More
950 Palladium: Superior White Color
Striking differences between elements such as color, tone, texture, reflection, refraction, pattern and shape create contrast. Contrast not only enhances...
Read More
American Holloware Changing Criteria
The expressions which have come to identify the pre- and post-World War II generations - Me decade, suburban frontiersmen, spoiled...
Read More
Revving Up the Burnout Process
The internet has put the world at our fingertips. In minutes or less you can start a video chat with...
Read More
950 Palladium Bridal Jewelry Manufacturing
Retailers have been converting bridal inventories from white gold to palladium as manufacturers expand the selection of new palladium jewelry...
Read More
William Underhill: Organic Geometry
William Underhill came to bronze pots just as his teacher at the University of California at Berkeley Peter Voulkos was...
Read More
950 Palladium: Stock Mountings and Findings
The reintroduction of white, bright and light palladium for use in the jewelry industry has quickly introduced an expanding assortment...
Read More
950 Palladium: Casting Procedures
With the jewelry industrys acceptance and increased use of new 950 palladium alloys for jewelry design and manufacturing, its fundamental...
Read More
Discussion on Refiner Methods
Shawna Kulpa takes a look into the assaying methods refiners use to determine the value of a lot. This article...
Read More
950 Palladium: Gemstone Setting
Setting gemstones in 950 palladium alloys is a bench jeweler'#39;s dream. Stone setters will agree that the combination of palladium'#39;s...
Read More
Lost Wax Casting Part 8 of 9 Cutting the sprues
This video was originally created to explain the casting process we use at Feathered Gems to the client whose charms...
Read More
950 Palladium: Fabricating Custom Earrings
This article examines manufacturing procedures used to hand fabricate 950 palladium earrings. These custom earrings designed by Lainie Mann feature...
Read More
Platinum Casting – The Platinum Expert – Episode 3
This video offers insight into the platinum casting process through five Platinum casting examples: two torch based casting and three...
Read More
Lost Wax Casting Part 1 of 9 Sprueing
This video was originally created to explain the casting process we use at Feathered Gems to the client whose charms...
Read More
How to Make Spiral-Cut Rubber Molds
In this installment we present a mold cutting technique called a spiral cut, which is designed to facilitate the successful...
Read More
Spiral Cut Technique for Rubber Molds
n this installment we present a mold cutting technique called a spiral cut, which is designed to facilitate the successful...
Read More
950 Palladium: Unique Manufacturing Process
This Unique Settings ring is an excellent design for palladium with heavy, low-profile prongs for the 1.50 carat center diamond,...
Read More
Hollowing Out A Wax Model For Lost Wax Casting
In this demonstration, a wax model is shown, and will be hollowed out from behind. A strong light is mounted...
Read More
Improved Anti-fire Scale Casting Procedure
This paper describes a process that eliminated fire scale during a vacuum casting cycle. Castings should not have a fire...
Read More
Lost Wax Casting Part 7 of 9 Cleaning the Castings
This video was originally created to explain the casting process we use at Feathered Gems to the client whose charms...
Read More
Water casting shibuichi
Casting shibuichi in the traditional japanese way on canvas in water.
Read More
Doneghy Collection of Southwest Indian Silver
At a time when the country is still reeling from the vogue for Indian jewelry displayed around the necks of...
Read More
Oval and Marquis Gemstone Layout Method
Accurately laying out an oval or marquis stone in wax can be tricky business. We learned this foolproof method for...
Read More
Ensuring the Best Refining Experience
Today's record metals prices have probably encouraged you to be more diligent than ever about capturing every last bit of...
Read More
Holts – Carve a cuttlebone mould for a stone setting
In this video, Nicholas of Holts Academy of Jewellery
shows you how to carve a cuttlebone for a stone
setting....
Read More
SACRIFICE
When there is no other way to solve the problem , it needs a sacrifice ...
Read More
Casting of small series of jewelry
Small scale centrifugal casting of jewelry
Read More
Lost Wax Casting – [6/9] Quenching the hot flasks
Lost wax casting, step : cooling the hot flasks in a bucket of water
Feathered Gems Jewelry has documented the...
Read More
RTV cylinder mold cutting of Akron rtv-rp
Mold cutting Akron RTV-RP clear silicone. Cylinder mold was cured in a round film canister which saves about 1/2 the...
Read More
Lost Wax Casting – [1/9] Sprueing waxes
Preparing for lost wax casting, step 1: attaching waxes to a central sprue and weighing them.
Feathered Gems Jewelry has...
Read More
Testing the CAD/CAM LMR Mold Compound
The new Romanoff LMR is a clear silicone RTV (room temperature vulcanizing) liquid mold rubber compound with a platinum-containing catalyst,...
Read More
950 Palladium and Tahitian Pearl Earrings
These 950 Palladium earrings were designed by Tom McLaughlin of Lennons Jewelers, Syracuse, NY. The top portion of the design...
Read More
Platinum Bridal Jewelry
If you have never manufactured with platinum and you think that you are ready, if you manufacture with platinum, but...
Read More
Casting
Video showing how the casting process is made.
Read More
950 Palladium: 22K Granulation Wedding Band
This band was designed and rendered using Gemvision Matrix jewelry
design software. The 22-karat granulation beads measure
approxiametely 1.0 millimeter...
Read More
cuttlefish bone casting
preparing the bone and casting a ring
Read More
Lost Wax Casting – [9/9] Finishing and Polishing
Lost wax casting, step : Grinding, buffing and polishing the finished charms.
Feathered Gems Jewelry has documented the entire process...
Read More
1983 SNAG Platinum Jewelry Design Competition
This year Johnson Matthey Inc., the world's largest manufacturer of platinum group metals, in cooperation with the Society of North...
Read More
Lost Wax Casting – [7/9] Cleaning the newly cast charms
Lost wax casting, step : cleaning the freshly cast silver charms.
Feathered Gems Jewelry has documented the entire process of...
Read More
950 Palladium: Making a 3-Stone Ring
When heated to high heat soldering temperatures, some 950 palladium alloys will develop a bluish-purple surface discoloration. It is easily...
Read More
Laying Out a Pattern In Wax With Kate Wolf
Creative Side Jewelry Academy of Austin presents Kate Wolf, owner of Wolf Tools, as she demonstrates how to more quickly...
Read More
5 Holiday Casting Process Tips
The hazy days of summer aren’t too soon to begin thinking of designs for the holidays—and how to best cast...
Read More
custom necklace part 7,, the last part
Making of a custom 10 y gold Versace link necklace, polishing and finished piece,,thanks blingbling.ca
Read More
cuttlebone molds
Ancient jewelry making technique using cuttlebone molds - Artisan jeweller, Eftihios Tsivourakis, demonstrates the ancient technique of mould-making using cuttlefish...
Read More
Lost Wax Casting – [8/9] Cutting the charms off of the sprue
Lost wax casting, step 8: cutting the now clean silver charms off of the sprue trees.
Feathered Gems Jewelry has...
Read More
Matt Miter Box-Cut Straight or Parallel Walls
A perfect wax model starts with a perfectly cut wax blank. With the Matt Miter Box (Matter Box) you can...
Read More
Create a Two-Color Casting
Combining the Matt Mini-Lathe and Matt Gun techniques to create a two-color casting.
Read More
Jewelry Designs: Maya Pendant
Welcometo Stacey Rhodes Jewelry Designs, where we will detail all of the steps involved in adding a new piece ofjewelry...
Read More
jewellery school perseo
La scuola professionale "Perseo": l'unico in Italia per la gioielleria, dove i proprietari sono tutti artigiani-artisti. Nato a Firenze nel...
Read More
Gold Casting Machine, Silver Casting Machine
Gold Casting Machine, Silver Casting machine,wax injector, die press, vulcanising press, wax, rubber, investment mixer, burn out furnace, jewellery casting...
Read More
Lost Wax Casting – [4/9] Burning out the flasks
Preparing for lost wax casting, step 4: putting the flasks in a kiln to burn out any remaining wax and...
Read More
Lost Wax Casting Part 9 of 9 Finishing the charms
This video was originally created to explain the casting process we use at Feathered Gems to the client whose charms...
Read More
Natural Rubber Mold Making Tools
Tools for making natural rubber molds.
Read More
Lost Wax Casting Part 2 of 9 Investing
This video was originally created to explain the casting process we use at Feathered Gems to the client whose charms...
Read More
VLT flat cut 7 circuit pendant
Flat cut silicone mold using Castaldo VLT rubber.
Read More
making a rotory file from a lighter
making a rotory file from a lighter flint wheel.
Read More
The Queen of the Night
This video documents the making of a silver necklace inspired by Mozart's "The Magic Flute". The green and purple material...
Read More
Jewelry Designs: Raindrops Pendant
Welcome to Stacey Rhodes Jewelry Designs, where we will detail all of the steps involved in adding a new piece...
Read More
Lost Wax Casting – [5/9] Casting the silver in the heated fl
Lost wax casting, step 5: weighing and melting the sterling silver that is poured into the hot flasks.
Feathered Gems...
Read More
Third Hand For Casting
A helpfull tip you can put together with a clamp from hardware store.
Read More
Versace necklace part 2
the making of a custom necklace
Read More
Lost Wax Casting Part 5 of 9 Casting the Silver
This video was originally created to explain the casting process we use at Feathered Gems to the client whose charms...
Read More
Lost Wax Casting Part 4 of 9 Burning Out
This video was originally created to explain the casting process we use at Feathered Gems to the client whose charms...
Read More
Making a fairy part two
Casting and finishing the fairy
Read More
Custom Necklace Part 5
The making of a custom necklace, artcam , modelmaster , casting, burn out , polishing,
Read More
Versace Custom necklace part 3
the building of a custom 10 k yellow gold necklace, artcam jewelsmith, and modelmaster cnc
Read More
Lost Wax Casting – [3/9] Dewaxing the flasks
Preparing for lost wax casting, step 3: steaming out the wax from inside the hardened plaster investment.
Feathered Gems Jewelry...
Read More
Custom Necklace Part 6
the casting polishing assembly of the 10 k yellow Versace custom necklace
Read More
Lost Wax Casting Part 6 of 9 Quenching the Flasks
This video was originally created to explain the casting process we use at Feathered Gems to the client whose charms...
Read More
Lost Wax Casting – [2/9] Investing the wax-filled flasks
Preparing for lost wax casting, step 2: putting the waxes inside steel flasks and covering them with high temperature plaster...
Read More
Tanzanite Ring part two
Casting and fabrication of 14k gold ring for Tanzanite.
Read More
Making a silver fairy
First video of wax work
Read More
Custom Necklace part 4
The building of a custom 10 k. yellow gold necklace,, artcam jewelsmith, modelmaster cnc, casting , burnout and stuff like...
Read More
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.