Bench Tips and Tricks
Our Bench Tips and Tricks section covers jewelry making and repairs. Get the most from your tools and materials, from mandrels to palladium to gems.
HomeBench Tips and Tricks
Make Your Own DIY Rotary Burr
Make your own high quality rotary burr from an inexpensive disposable lighter. By master goldsmith Charles Lewton-Brain. Filmed in full...
Read More
How to Harden and Temper Tool Steel
Learn to harden and temper your own custom-shaped jewelry tools. By master goldsmith Charles Lewton-Brain. Filmed in full HD 1080p....
Read More
Step by Step Guide to Single Row Pave Settings
Single-row pavé, which consists of a single row of small diamonds set into a narrow strip of metal, is a...
Read More
Other Uses for a Pencil in Jewelry Making
Two surprising uses for a pencil as a tool in jewelry making. (1) Gain extreme control over the burr on...
Read More
Make Your Own Cardboard Disc Sander
Handy trick to make a useful cardboard disc sander which master goldsmith Charles Lewton-Brain learned about at a factory in...
Read More
Method to Quickly Identify Tool Steel
Learn to be able to quickly identify what quality of steel a tool is made of and whether it's low...
Read More
How to Repair a Hollow Rope Chain
I took in a broken hollow rope chain bracelet for repair this week. The bracelet had caught on a desk...
Read More
The Best Flux For Soldering Jewelry: How To Choose The Right One For Your Project
Technical Briefs deals with technical concerns of interest to a wide audience, addressing topics as diverse as vanguard technology and...
Read More
How to Create a Basic Link Chain
Making a simple or basic link chain to display your pendant designs is a great way to add further value...
Read More
Dealing with Fire Scale
Fire scale or fire stain is a reddish purple toned 'bloom' or 'stain' that appears on silver/copper alloys such as...
Read More
Tips & Techniques for Popular Finishing Touches
We asked a number of top jewelers to tell us their best practices, techniques, and tips for creating satin, brushed,...
Read More
Basic Spiral Braiding
[Step by Step] This five-strand spiral braid is made using one of the many textile techniques that Professor Arline Fisch...
Read More
Jeweler’s Saw Blades: All The Different Sizes And How To Choose Correctly
Originally published under the title: Selecting the Correct Saw Blade
This article provides and describes useful tips for selecting the...
Read More
Box Clasp Fabrication
One of the most important types of closures used in jewelry is the box clasp. This clasp and its many...
Read More
Hammering and Forging Safety Guidelines
Goldsmiths and silversmiths use hammers frequently in their work, silversmiths especially. A regular trade goldsmith might use a bench hammer...
Read More
Enameling Techniques for Beginners
After you learn to apply enamels by sifting, wet packing, brushing on crackle and firing the base coats, you are...
Read More
Electroplating Safety Precautions
The "General Safety Rules for Tools" article applies here too, as with all power tools. Read the instruction manuals and...
Read More
Build a Basic Jeweler’s Bench
This bench has been designed so it can be made from easily available materials without sophisticated woodworking equipment. People with...
Read More
Important Principles of Casting Safety
Here's something to aim for: a well laid-out, orderly workshop, well-lit by multiple non glare light sources, well-maintained equipment, electrically...
Read More
Soldering Hints and Tricks
Medical hemostats and forceps make good clips for wire solder. Soldering clips for soldering work may be made from cotter...
Read More
Creating and Sharpening Gravers
This article is about creating and sharpening gravers before using for your work or project as described by Tom Weishaar....
Read More
3 Ways to Use 2-Part Epoxy Resins
Available in a wide variety of formulas, epoxy resins are used in jewelry making as adhesives, as coatings, and for...
Read More
A Metalworking Hand Tool List For Beginners In Jewelry-Making
Making jewelry is sometimes seen as a difficult or an expensive proposition. In reality a basic metal working shop can...
Read More
Textile Techniques in Jewelry Making
Fabrics and precious metals would seem to be total opposites, like hot and cold or yin and yang. However, despite...
Read More
Pickling Notes
Jewelers treat soldered objects with dilute acid solutions to remove oxides produced from heating and soldering as well as glassy...
Read More
Tips on How to Master Soldering
Soldering is probably the most commonly used and least understood operation performed in the jewelry industry. Most jewelers know how...
Read More
Basic Filing Techniques
Over the years, bad habits creep into our work procedures. Periodical review of our techniques is needed to assure us...
Read More
Basic Polishing Technique
Many jewelers see polishing as a mundane task. However, it is one of the most important operations in the process...
Read More
950 Palladium Bench Guide
The palladium bench guide reviews the working characteristics of palladium for the jewelry bench staff and provides an overview of...
Read More
Patination Safety Considerations
Jewelers use so-called -oxidising- solutions to darken metals like silver, copper, brass, nickel silver, bronze and, with specialized mixtures, on...
Read More
How to Make Hoop Earrings
Tom Dougherty of Studio 2015 in Woodstock, Illinois, had an interesting process to share about making hoop earrings from tubing....
Read More
Platinum Durability vs Scratching
There is a major difference between durability and scratch resistance. Platinum is very durable. When scratched, the scratch actually displaces...
Read More
Casting Investment Materials and Applications
The casting investment process enjoys wide popularity in the production of commercial and one-of-a-kind art metal objects. However, production practice...
Read More
How to Make Earring Posts by Hand
Yes you can make your own earring posts. It is generally more cost effective to buy them, but making them...
Read More
The Art of Anticlastic Raising
Transforming a single sheet of metal into an undulating organic form using only a hammer and stake is the art...
Read More
Channel Setting – Set ‘Em Straight
Over the past decade, channel setting has grown in popularity. Setting small diamonds, rubies, sapphires, and even emeralds into channels...
Read More
Jewelery Workshop Ventilation
Ventilation means removing noxious materials, dusts and fumes from where you can breathe them in. It is about taking away...
Read More
Making Your Own Tubing
Not all sizes and wall thicknesses of tube come seamless from a factory or refiner. Especially when working in gold...
Read More
Basic Bead Setting Techniques
First the stone's diameter is measured at the pavillion and a dent is made in the metal for the pilot...
Read More
Differences between Managing and Micromanaging
As a Business Strategy it is important to recognize the differences between managing and micromanaging. Read on for Andrea Hill's...
Read More
The Best Jewelry Books: A Comprehensive Reading List For Craftspeople
A selected bibliography list for the jeweler - Metal working, Casting, Plating, Enamelling ,Gem Cutting, Setting, Engraving and Etching, Other...
Read More
Platinum Jewelry Advanced Joining Techniques
Joining is a very important production technique in the field of jewelry production. Therefore it is useful to know, what...
Read More
Working with Pearls
Both natural and cultured pearls are formed when an irritant lodges in a mollusk. The mollusk then deposits layers of...
Read More
International Ring Sizes Chart
This page provides an international ring sizes chart you can view and/or download to be your guide in making or...
Read More
Knowing the Difference Between Carat and Karat
Carat, karat, caret, and carrot are all pronounced the same, but each has a different meaning. Carat and karat, of...
Read More
Potentially Harmful Metalsmithing Substances
In every aspect of my daily life I am, and have been for quite some time, concerned with promoting and...
Read More
The Costs of Learning Hand Engraving
When you've made the decision to learn hand engraving, you have basically 3 options: Spend little or no money but...
Read More
Dusts in the Jewelry Workshop
Dust is small particles of a material. There are dusts you can see in the air; these can be breathed...
Read More
Gemstone Exploration Techniques
The most widely-used gemstone exploration techniques today are ground-penetrating radar, known as GPR; trace-element analysis, which involves seeking signature elements...
Read More
Tips and Tricks for Scoring Metal
Scoring metal is incredibly important for custom jewelry construction. It enables you to reduce the number of parts in a...
Read More
20 Laser Welding Tips
This article offers some laser welding tips that might make your life as a laser welder a bit easier. Read...
Read More
Gem-Setting Tools: A Practical Guide To All The Hand Tools & Bench Supplies You’ll Need
This article lists the basic tools someone learning stonesetting might want to have around. One would of course add to...
Read More
Bi-Metal Casting to Titanium
Titanium and the other refractory metals other the metalsmith a new range of exotic colors - colors that are beautiful...
Read More
Quality Assurance Benchmarks for Jewelers
Fine jewelry represents much more than its trade value in diamonds, gemstones and precious metals. It is a personal representation...
Read More
Working with Topaz
The primary issue with topaz that must be remembered at the bench is its one perfect cleavage direction. Hammering or...
Read More
Methods to Effectively Bend Tubing
Jewelers need to bend tubing for various constructions, including neckpieces, earrings, catches, and cuff links. Normally, precious metal tubes are...
Read More
A Metalsmith’s Guide to Los Angeles
This Metalsmith's Guide to Los Angeles can be useful to metalsmiths who are new to the Los Angeles area or...
Read More
Debunking a Soldering Myth 1
After 25 years as a jeweler, first as a student, an apprentice, an instructor, and now a master instructor and...
Read More
Basic Sawing Techniques
In this article, we will continue our Back to Basics Series with an article on Sawing techniques.
Read More
Cutting Jump Rings
Once you've wound jump rings around a mandrel, what's the best way to cut them apart? Some craftspeople use hand-held...
Read More
Metal Conversion Chart
The metal conversion chart below will help you determine the amount of metal needed to create a piece of jewelry...
Read More
Step-by-Step Guide to Upsizing Rings
When I ran a trade shop, time was money, and I often found myself sizing 50 to 60 rings in...
Read More
Comparing Buff Prep Methods
Myth: Singeing buffs to prep them is faster and more effective than raking them.
There are as many people in...
Read More
Bezel Setting Method
Bezel setting is one of the most secure methods of setting a gemstone into a mounting, but one of the...
Read More
Notes on Presto-Lite Torch
We use a method for cutting down firescale when using a Presto-Lite Torch along with an acetylene B tank. The...
Read More
Grinding Wheel Safety Rules
Besides the safety instructions that you get from a tool manufacturer in the tool manual it may be necessary for...
Read More
Lapidary Work Safety Precautions
Goldsmiths sometimes do a little rough and ready lapidary work with emery and leather sticks or even polishing compounds on...
Read More
Working Posture for Craftsmen
Many craftspeople have posture and body position problems. Ramazzini, the founder of occupational medicine and author of a groundbreaking book...
Read More
Jewelers Saws Tested: A Hands-On Review Of The Knew Concepts Precision Lineup
I have an intimate relationship with my tool collection. Sometimes the needs of a particular jewelry project drive me to...
Read More
Royal Flush Stone Setting
A sign on the side of a plumbers truck read, In our business a Flush is better than a Full-House....
Read More
Gemstone Care Tips
Many gemstone owners enjoy wearing their treasures. Few things can ruin that enjoyment faster than the discovery of damage such...
Read More
Polishing Hard to Reach Areas
When it comes to fine jewelry making polishing is a very important step - it can be the difference between...
Read More
Basic Safety Principles for Jewelers
Aim for: a well laid-out, orderly workshop, well-lit by multiple non glare light sources, well-maintained equipment, electrically and fire safe,...
Read More
How to Resize Platinum Rings
This article offers instructions on how to resize platinum rings whether for a size smaller or bigger, as well as,...
Read More
Setting Stones in Wax
One of the most revolutionary advances in recent years, apart from laser welding, is the method of setting stones in...
Read More
Gloves and the Jeweler
Gloves are used to prevent skin contact with a hazard, whether physical (like a razor edge on a piece of...
Read More
Beading Tool Tips
Like most bench jewelers I do a lot of bead setting and like most
bench jewelers I take pride in...
Read More
Basic Setup for Jewelry Photography
A vertical copy stand is sometimes used for shooting prints, drawings, jewelry and other fairly flat objects. A copy stand...
Read More
Re-tipping Platinum Prongs
Platinum is a very durable metal, so prongs will last a long time. However, it is sometimes necessary to re-tip...
Read More
Goldsmithing Health Hazards
This article briefly reviews issues of studio safety and discusses ways of recognizing risks in the studio and reducing hazard...
Read More
Hydraulic Press Safety Precautions
Goldsmiths began to use hydraulic presses in small shops in the 1940s in North America. Factories have used hydraulic presses...
Read More
Notes on Files for Jewelry Making
When one gets a new file one traditionally dips it in alcohol and sets fire to it to burn off...
Read More
Jewellers’ Objective Attitude Towards Designing
It is sometimes useful to have criticism of one's work in order to develop it. While studying as an apprentice...
Read More
Securing Curved Stones for Easy Drilling
Securing curved stones when drilling can be a bit difficult. I use recycled ceramic china, beach pebbles, sea and river...
Read More
Methods of Closing Jump Rings
In high volume production operations, many jump rings need to be closed one after another. For such fast paced operations,...
Read More
CAD/CAM: The Basics
What if you could sit down at your computer, spend a little time manipulating the mouse, keyboard or electronic pencil...
Read More
How to Make an Ionic Cleaner
Although ultrasonic cleaners are great for removing gunk on jewelry, they do a poor job when it comes to removing...
Read More
Laser Repair: Bangle Bracelet
It's an "everyday" kind of repair job. The customer brings in a bangle bracelet that has a broken safety slide....
Read More
Project Management for Jewelers
I came up with this system to solve some production and prioritizing problems at a small custom jewelry store. We...
Read More
Jeweler’s Workday: Sitting and Looking at the Bench
In the Jewelers Bench Book, the MJSA/Ganoksin project published in spring 2008, there is an extensive look at what happens...
Read More
Palladium Annealing and Soldering
If you're just starting to work with palladium or interested in taking the leap, you should know a few critical...
Read More
What to Know About Heavy Metal Testing
Before you submit any jewelry item to a lab to test for heavy metals, you're going to need to do...
Read More
6 Basic Wire Skills to Make a Necklace
The links in this 16-in. (40.6cm) necklace are forged so they become flat and work-hardened. The pearl in the featured...
Read More
Dermatitis and the Jeweler
Dermatitis is a group of skin conditions that may often be contracted by exposure to chemicals and metals. These may...
Read More
Tips on Working with 35mm Slides
A note on slide developing: you want your slides to be developed for the best quality possi¬ble. If you want...
Read More
Choosing the Right White Gold
The popularity of white gold has us all looking to the most perplexing gold we use. Perplexing a variety of...
Read More
Tips for Recovering Precious Metal Particles
Most jewelers know how to handle their precious metal scraps: they separate their scraps by metal, dry out ultrasonic solutions...
Read More
Magnesia Blocks Myth Debunked
Myth: Magnesia blocks are superior soldering surfaces to charcoal blocks: A topic that seems to raise a fair amount of...
Read More
Perfectly Fit Bezel
Joints that fit well make soldering a snap. The next time you need to solder or fuse a bezel, try...
Read More
V Prong Setting
Several shapes of stones have pointed ends, including marquise, pear, heart, and princess. Because these points are often thin and...
Read More
Making Wooden Raising Stakes
This article offers a few tips on making your own wooden raising stakes instead of buying rather expensive metal ones....
Read More
Tips for Avoiding Meltdown
Now What?
You’ve carved a few waxes or made a piece in metal that you want to mold and have...
Read More
How to Sharpen Drill Bits
Small, fine drill bits used for jewelry making will become dull with normal use. Worn cutting edges make tasks more...
Read More
Sneaky Goldsmith Tricks
The best 'Sneaky Goldsmith Tricks' involve taking mundane, everyday items and repurposing them as goldsmith's tools. Two classic tricks that...
Read More
Copper Granulation Technique
Granulation, a technique used in jewelry and metalwork, is the decorative use of minute metal granules attached to the surface...
Read More
Drilling Tips and Techniques
We all drill, all the time. We take drills and what they do for granted, but reviewing the obvious doesnt...
Read More
Basic Fire Safety for Jewelers
Have a fire plan; ask your fire department for advice. Keep the appropriate extinguishers around and in good shape. Get...
Read More
Gas Handling Guidelines
Jewelers work with compressed gases of all kinds, in torch systems, kilns, casting machines, abrasive blasters, laser welding machines needing...
Read More
Making a Metal Brooch Frame
This is a metal frame for a brooch which can be made without any soldering. Findings can be glued or...
Read More
Safety Notes for Jewelers on Pitch, Chasing and Repousse
An ancient system of working metals, this procedure uses steel punches to manipulate the metal while it is fixed onto...
Read More
Repairing Broken Chains
The difficulty of chain repair lies in the fact that the chain is made up of fine wires. These wires...
Read More
Palladium Q&As
Its no secret that palladium has captured the attention of the industry. In 2005, purchase of palladium for jewelry use...
Read More
Ring Sizing Tips and Tricks
Ask a seasoned bench jeweler how many rings he or she has sized and they'll probably give you a figure...
Read More
2 Successful Stone Setting Tips
Ask any experienced jeweler, and they'll tell you: it takes stones to become a gem setter. You literally have to...
Read More
DIY Metal Shaping Tools: How To Make Your Own Jewelry Hammers Or Mallets
Jewelers spend hours fixing damage that they themselves did to the metal. Soft hammers and shaping tools limit the injuries...
Read More
Communication for Customer Satisfaction
In the quest to get some insights into designing and marketing customized jewelry "customer whisperers" agreed that communication is the...
Read More
A Pain In The Neck
You start to turn and there it is again. You go to stand up from your chair and it happens...
Read More
Chain & Findings
This segment from the 2017 MJSA Journal November issue is dedicated to metals, tools, software and more that aids jewelers...
Read More
Debunking Three Myths About Sawing
In thinking about the daily tasks that I undertake at the bench, I realized how easy it is to fall...
Read More
Touchstone Method for Testing Karat Gold Purity
There are a few scientific methods for precisely determining karat gold purity, some destructive (fire assay) and others nondestructive (X-ray...
Read More
Using Dental Mold-Making Materials
Jewelers are always molding objects and parts, most often to use for making wax models for casting. There are many...
Read More
A Metalsmith’s Guide to Washington, D.C.
This is a continuing series of metalsmith's guides to cities, regions and museums throughout the world. The purpose of these...
Read More
Prong Setting & Ring Sizing Tips
I'm going to do something different in this issue. Instead of taking you through the steps involved in putting a...
Read More
Tips for Repairing Pearl Jewelry
When taking in a piece of pearl jewelry for repair, it may be necessary to remove the pearl to avoid...
Read More
Build an Advanced Jeweler’s Bench
This sophisticated bench costs a little more and is a bit more difficult to make than the one on the...
Read More
Platinum Finishing/Polishing Process
Opinions differ considerably when discussing the ease or difficulty of polishing platinum, but most agree that when a piece is...
Read More
Rendering Design and Process
This is the second in a series of articles on the art and skill of rendering jewelry and small metal...
Read More
What Causes Casting Marks?
In the Spring 2003 Issue we asked the question "What causes these marks on this casting?" Around 100 readers responded...
Read More
Making Hollow Forms in Carving Wax Using Bread
White, gummy Wonder Bread isn't just for peanut butter and jelly sandwiches. It's a fun tool for making hollow forms...
Read More
Tweezers Tips and Tricks
Tweezers are a constant in a jeweler's life, particularly in these safety conscious times. Tweezer use can help reduce your...
Read More
Photoetching for the Studio Jeweler
In photoetching a photo transparency defines the area of a metal plate to be etched. The transparency is the control...
Read More
Basic Principles for Tools and Equipment
Saving some dollars on equipment can be really helpful to a shop's bottom line. Often tools and equipment from other...
Read More
Roll Printing Technique
Roll printing, or texture transfer, has been around a long time. The ancient Greeks and Romans used various dies and,...
Read More
Flexible Shaft Tricks
A good selection of burs may be had from your dentist. Dentists often throw out burrs which still have a...
Read More
Transform Nails To Riveting Tools
Soldering is a quick and easy method for joining metals. But sometimes two metals require a connection for which soldering...
Read More
How to Make a Riffle File
Every now and then when you are fabricating a piece or polishing a casting, a hole or hollow will pop...
Read More
Fit to be Sized
Before sizing any ring, examine it carefully and compare it to the information on the job envelope. If you see...
Read More
Practical Wax Modeling Techniques
To begin with I highly recommend this book of technical information and procedures for anyone wanting to learn wax modelling...
Read More
Giving New Life to Old Burs
By Old burs can serve a number of useful purposes in daily bench work. Here are two tips from jewelers...
Read More
Useful Bench Tools
This segment from the 2017 MJSA Journal November issue is dedicated to metals, tools, software and more that aids jewelers...
Read More
CAD/CAM Techniques
The strength of Computer Aided Design & Manufacturing is similar to that of any other tool on the bench:it is...
Read More
Color Coding Solder Chips
Let's face it, not every snippet of solder winds up in your work. Some pieces fly away during clipping, while...
Read More
Fabricating a Crown to Fit a Stone
Often jewelers are called upon to hand fabricate a crown to fit a stone. This is necessary when either the...
Read More
Organize Your Bench
The next time you sit down at your bench, don't think of it as just a bench. Think of it...
Read More
Noise and its Effects
Noise is so common that we don't tend to think of it in terms of exposure in the same way...
Read More
Platinum Fabricating & Stamping
This paper is aimed mainly at the small- to medium-sized jewelry manufacturing operations interested in working with platinum group metals....
Read More
Carpal Tunnel Syndrome, other RSIs and the Jeweler
Carpal tunnel syndrome is only one of many kinds of repetitive strain injuries (RSIs) and cumulative trauma disorders (CTDs). RSI,...
Read More
Tips for Creating Jump Rings
Jewelers use jump rings extensively as chain components, connectors, and linking devices for multiple construction problems. Here are a few...
Read More
Translating Line Art into 3D Models in Matrix
Line art, such as logos, family crests, text or numbers, cartoon characters, and even sketches can be quickly and easily...
Read More
Casting Tools and Products
This segment from the 2017 MJSA Journal November issue is dedicated to metals, tools, software and more that aids jewelers...
Read More
Inside Ring Polishing
Trying to get a really high polish on the inside of a ring can be frustrating. Because inside ring buffs...
Read More
Perfect Finishing Tools and Techniques
Our castings can be flawless, our assembly precise, and our settings secure -- but let any surface go a bit...
Read More
North American Sources for Equipment, Materials, etc.
This page offers a list of some useful North American Sources for Equipment, Materials, information, etc that would be very...
Read More
CAD/CAM Designer Tools
This segment from the 2017 MJSA Journal November issue is dedicated to metals, tools, software and more that aids jewelers...
Read More
Bezel Setting Cabochon Stones
One of the most basic designs in stone setting is Bezel Setting. It is rudimentary in its concept, and it...
Read More
Gemstone Chemical Coloration Techniques
The most important detail in the preparation of gemstone for chemical coloration is that it be clean. Oil and grease,...
Read More
Transparency Making for Photoetching
This article, "Transparency Making for Photoetching", is the first of two parts written by Allan Liu and Carol Webb. Check...
Read More
Stone Setting Tips
Here are some very helpful stone setting tips provided by Gerald Lewy to help and guide you when working on...
Read More
Palladium Sizing, Welding and Engraving
In this article Chris Ploof shares tips for sizing, welding, and engraving palladium.
Read More
Basic Milling Technique
In working on jewelry there are many tasks that seem simple - you just do it and don't think about...
Read More
Avoiding Melting Soldered Seams
Soldering is a delicate and sometimes difficult process especially when you need to solder very close to a previous solder...
Read More
Bench Tools for Jewelers
This article lists the following useful bench tools for jewelers including contact information where they can be purchased or ordered....
Read More
Radial Bristle Discs Excites Jewelers
how one of 3M's radial bristle discs to a non-jeweler friend, and you are almost guaranteed to get a lukewarm...
Read More
Paraffin Wax Treatment
The holiday season can be rough on jewelers. The long hours spent toiling at the bench trying to fulfill last...
Read More
Bench Tips and Tricks of the Trade
To stretch a wedding band that is larger than your ring stretcher mandrel, slip a copper sleeve over the mandrel...
Read More
Graver Detailing and Sharpening
A sharp graver can improve cutting performance at the bench. There are several approaches to use when detailing a graver,...
Read More
Handling Colored Stones at the Bench Part 2
I’m hoping this series of articles will save some of you time, money, and embarrassment by discussing some of the...
Read More
Firescale Prevention During Vacuum Casting
Firescale has been the scourge of sterling silver casters since the first silver was poured into a mold. It has...
Read More
Using Non-Jeweler’s Tools For Fabrication: How To Repurpose Painting Blades For Bezels
Helen I. Driggs demonstrates how some non-jewelers tools give fabrication a new twist.
My background is in graphic design, so...
Read More
Layout Form / Template
Click on the image to enlarge and download and you can use this layout form or template to help layout...
Read More
Art vs Craft
The Art versus Craft issue is a complex question and one that has bedeviled creators a great deal in the...
Read More
Bezel Setting Using a Lathe
Bezel setting the center sapphire is normally pretty straight-forward, but I would like to share a few tricks that have...
Read More
All About Jump Rings
Jump rings may be made most easily by using a small hand drill with various sizes of mandrel. Take a...
Read More
A Metalsmith’s Guide to Tokyo, Japan
Nothing is simple in Tokyo—not the language, not the culture, not the geography. Even getting information is a major task...
Read More
A Conversation with Michael Rowe
Michael Rowe uses functional containers as a base from which to explore formal studies of space, form and balance, which...
Read More
Studio Lighting Considerations
How you light your shop, illuminate your working area, experience the reflection from surfaces and the paint you choose for...
Read More
Tips for Modifying Vises
A good vise is a vital piece of equipment for any goldsmith because it can act as a third hand,...
Read More
How to Mount Objects in Metal Frames
For the illusion of "floating objects" Helen I. Driggs shares her technique, a step by step guide, on how to...
Read More
Proper Studio Light
Do not get caught in the dark - make certain your shop is well lit. In the jewelry shop, two...
Read More
Contemporary Applications of Area Inlay
The use of area inlay, called damascening or woven inlay, is common in the ancient metalwork of Iran, India, Japan,...
Read More
Bead Setting Method – Part 3
In past issues of BENCH magazine, I have dealt heavily on making a bead raiser and using it to bead...
Read More
How to Make a Bezel
There are several ways to make a "box-setting" for enameled work pieces. This is one way on how to make...
Read More
3 Top Challenges for Jewelry Makers in 2014
Editor's Note: Looking ahead at the coming year, it's just as important to consider the challenges facing the jewelry industry...
Read More
Platinum Bench Tricks
This project is dedicated to bench tricks that make working with platinum-or working at the bench in general-easier. This is...
Read More
Using Coils To Bend Tubing
Many tools sold in model/hobby stores can be used for jewelry making. During a recent visit to a hobby shop,...
Read More
Creating Beading Pliers Accessory Bezel Settings
Sometimes, holding on to really little parts is the greatest challenge of my day. I use tiny cabochons almost daily...
Read More
Technical Briefs: Dealing with Firescale
Technical Briefs deals with technical concerns of interest to a wide audience, addressing topics as diverse as vanguard technology and...
Read More
Display & Packaging
This segment from the 2017 MJSA Journal November issue is dedicated to metals, tools, software and more that aids jewelers...
Read More
New Efficient Bench Applications
Pre-finishing, finishing, polishing and re-finishing have all been tasks usually done with a flexible shaft at the bench and/or a...
Read More
Creative Uses for Duct Tape at the Bench
Ask any bench jeweler the best way to secure a band-aid to his or her cut finger during a day...
Read More
Art and Technics: Technical Mastery
This article is one of a series of articles from Metalsmith Magazine “Art and Technics” talking about techniques in craftsmanship...
Read More
Practical Approach to CAD/CAM
Once more the realm of engineers and number-crunchers, CAD over the years has become more user-friendly and artisan-intuitive. Similarly, small-shop,...
Read More
Craftsmanship Improvement Method
This is a method to reduce technical problems which one repeatedly experienes. We all find during the learning process that...
Read More
How to Make Sharp Corner Cuts
Sawing is an essential skill for a bench jeweler. This article will show you a technique that will increase your...
Read More
Overcoming Bench Mistakes
From the Editor: It’s happened to everyone. You’re working on a project and everything is going along well until…. Oops....
Read More
Safer Pickle Alternative
Procrastination can sometimes lead to wonderful discoveries. Tom Arnold, owner of Facets Fine Jewelry in Arlington, Virginia, found this out...
Read More
Using Acid Bath on Used Tools
Bench jewelers hate to throw out used tools. By training and by nature we try to conserve the materials we...
Read More
Ergonomics for Bench Pin Modifications
Ergonomics is the safe and effective relationship between a worker and the work environment. For the bench jeweler who spends...
Read More
Tricks for Hollow Rings with Miniature Stakes
Make the inner band the desired size first. 18 or 20 gauge is about right. Next make the bezel or...
Read More
Tip for Improving Casting Quality
Every caster has seen his or her fair share of investment inclusions. You'll be polishing a casting when suddenly a...
Read More
Kinds of Alloys
This segment from the 2017 MJSA Journal November issue is dedicated to metals, tools, software and more that aids jewelers...
Read More
Cardboard Disc Sander Tool
A cardboard disc sander is a very useful tool. One uses the side or large flap of a fairly rigid...
Read More
Separating Work and Home
Often craftspeople start out making craft objects in their living space, a kitchen, a living room, and sometimes continue working...
Read More
Goldsmith Jewelry Finishing Trick
Every bench jeweler has experienced the frustration of trying to sand and polish a nearly inaccessible area on a piece...
Read More
Flat Topped Solitaire Setting
The Flat Topped Solitaire Setting is a popular style setting that is slightly more complicated to set than the standard...
Read More
Tackling Chain and Finding Repair
Ask most jewelers about repairing a chain or finding and they’re likely to offer you their best Charlie Brown impression:...
Read More
Business Software Tools
This segment from the 2017 MJSA Journal November issue is dedicated to metals, tools, software and more that aids jewelers...
Read More
Modified Split Mandrel for Finishing Round Bezels
A bench jeweler typically uses a split mandrel to sand and finish the inside of a ring. Various grits of...
Read More
Fabricating a Free Form Opal Pendant
I received this opal from a woman who had cut it years ago. Her customer was aware it had a...
Read More
Rules for Tools
While it is clearly impossible to give a set of rules for each tool and procedure that goldsmiths use, this...
Read More
Methods for Applying Patination Solutions
Extremely clean metal surfaces give better results. See the article on Cleaning metal Surfaces for more information on cleaning.
Read More
New Gem Identification Techniques
This is an exciting era for gemologists. High-tech analytical techniques now make it possible to identify trace elements, treatments, and...
Read More
Organize Your Workspace
How you set up your shop, your working procedures and workspace can affect your safety, comfort, stress level and efficiency...
Read More
Handling Stakes and Anvils
Shaping a bezel on stakes is a process of forming the metal by stretching. First the metal is bent with...
Read More
Homemade Flex-Shaft Guard
Homemade flex-shaft guard using a soft drink plastic bottle, a solution to the annoying and potentially hazardous problem of breathing...
Read More
Jewelry Making Bench Tips
Jeremy Pavlow shares his common jewelry making bench tips by taking advantage of other tools and materials not normally used...
Read More
Jewellery Repair
Repairing jewellery is an extremely tricky job. Work often pretends to be something else, metal is not what it is...
Read More
Bench Tools Maintenance Schedule
Take a look around you. Chances are there is a flex-shaft or a dust collector you've neglected because you've been...
Read More
Discussion on Refiner Methods
Shawna Kulpa takes a look into the assaying methods refiners use to determine the value of a lot. This article...
Read More
Reusing Broken Saw Blades
Traditionally trained jewelers often scoff at the idea of using glue as a joining method. However, there are times when...
Read More
Photographic Images on Refractory Metals
The following article explains photo techniques used to transfer images onto refractory metals. These findings were developed during my graduate...
Read More
Creating a Rotary Burnisher
Jewelers have been going green for many years by recycling old or worn-out tools into something new and useful. Setting...
Read More
Overcoming Tool Limitations
True tales of how jewelers overcame out-of-the-box limitations - Most people who work with their hands become tool mad, and...
Read More
Book Review – Modeling in Wax for Jewelry and Sculpture
My first reaction when I heard about this book was, "It's about time." Think of it: If you tried to...
Read More
Technical Briefs: Fire Stain on Brass
Technical Briefs deals with technical concerns of interest to a wide audience, addressing topics as diverse as vanguard technology and...
Read More
Basic Approach to Product Design
Design is a perennial issue for all who produce objects meant for a specific use, utilitarian, in contrast to objects...
Read More
Tool Alterations
This article describes the different tool alterations that any bench man needs to know and learn as guidance for their...
Read More
Thai Chaser Tool Tricks
I was recently in Chiang Mai, a city in northern Thailand, where I spent a month visiting silversmiths and chasers...
Read More
Making a Multi-Grit Sanding Stick
BW Simon in Spartanburg, South Carolina, made this handy tool for finishing jewelry. I would like to thank him for...
Read More
Diamond Setting Hints
When setting a series of diamonds in a row, I use a 156C and just touch the inside wall of...
Read More
Hints on Making Tubing
This article is an extract from the book 'Hinges and Hinge-Based Catches for Jewelers and Goldsmiths'
Not all sizes and...
Read More
Design Layout Tip
Designing stock pieces for my jewelry store has never been more fun than it is now that I have a...
Read More
Platinum Consideration Factors
Jurgen J Maerz of the Platinum Guild International USA outlines factors to consider when adding platinum to your line of...
Read More
Millimeter Gauge Layout Technique
Meticulous planning and tedious layout are a big part of a goldsmiths life at the bench. It usually pays dividends...
Read More
How to Step-Roll Wire
One requires a taper on the end of the wire to grip it with when placed through a drawplate for...
Read More
Technical Briefs: Understanding Sandpaper
Technical Briefs deals with technical concerns of interest to a wide audience, addressing topics as diverse as vanguard technology and...
Read More
Organize Bench Workflow with Trays
There are numerous mass production processes that bench jewelers can adapt and use to streamline their studio jewelry work. One...
Read More
Managing Quality Problems
When I was in grade school, I decided to enter a gardening contest for 4H. Though I had experience helping...
Read More
The TAO of Bur Goodtip
Bur Goodtip, a legendary bench jeweler shows how sometimes a tool is not just a tool... We are taking a...
Read More
Diamond Setting Applications
What is one of the causes of a "rippling or jagged" effect around an inside cutting edge in a Gypsy...
Read More
Bead Stone Setting – Bead It!
Bench Jewelers often use different methods to accomplish the same work. I believe the end results are what is important,...
Read More
Handling Colored Stones at the Bench Part 1
Ever since childhood, I’ve been fascinated by rocks and gems. I started cutting cabs more than 40 years ago, and...
Read More
Art and Technics: Experience
This article is one of a series of articles from Metalsmith Magazine “Art and Technics” talking about techniques in craftsmanship...
Read More
Half-Ground Round Bur
There are times during the setters workday where there is a need for a specific tool, but there nothing is...
Read More
How to Refuse Big Orders
Refusing a big order may sound like a business mistake, but sometimes saying no pays. Sales do not equal profit,...
Read More
Spiral Cut Technique for Rubber Molds
n this installment we present a mold cutting technique called a spiral cut, which is designed to facilitate the successful...
Read More
Evenly Heating Pieces for Soldering
One of the most difficult aspects of soldering is to heat the piece properly so that the solder will flow....
Read More
Jewelry Making Tricks
Check out this list of 19 jewelry making tips and tricks for preparation, cleaning, setting, how-to's and more.
Read More
Structuring for Efficiency in the Studio
Being more organized, and planning how you use your time will mean that you will spend less time on some...
Read More
Gemstone Setting Tip: Shape
“You should know what kind of shape you’re in,” joked Arthur Anton Skuratowicz during an MJSA At the Bench Live...
Read More
Creating a 14KW Rubellite Tourmaline Pendant
Steve Satow describes the procedure on creating a 14KW Rubellite Tourmaline Pendant.
Creating a 14KW Rubellite Tourmaline Pendant
Beginning components...
Read More
Debunking a Soldering Myth 2
There are many myths about heating pieces during soldering that can cause innumerable problems during relatively simple soldering operations. In...
Read More
Customized Mini Clamp Tool
I like to hold small pieces of metal with a clamp that allows me to file hands free. I feel...
Read More
Customized Earring Setting Pliers
Steve Satow shows the procedure for a customized earring setting pliers using a normal setting pliers.
Normal setting pliers can...
Read More
Locating Dead Center on Ring Blanks
This article provides a helpful tip on locating dead center on ring blanks and finding balance on an object.
Free-form...
Read More
Resizing Damaged Rings
This page provides some helpful tips when it comes to resizing damaged rings with stones. Read on for more.
When...
Read More
Knife Making Techniques for Jewelry Design
My dad was in the Navy during World War II and was among the personnel who entered Japan shortly after...
Read More
Oval and Marquis Gemstone Layout Method
Accurately laying out an oval or marquis stone in wax can be tricky business. We learned this foolproof method for...
Read More
How to Modify Prong Pushers
Many stone setters would agree that one of the most challenging aspects of prong setting is getting the prongs down...
Read More
Administering a Client Personality Test
When working with a client to discern their personal style, do you ever administer a personality test? If not, you...
Read More
Vector Tightening to Secure Gemstones
Gemstones that become loose in their settings can cause damage to both the gem and the setting. A regular inspection...
Read More
The Value of Ideas on Metalsmith/Jeweler’s Repertoire
This essay originated as a presentation at the Society of North American Goldsmiths’ conference in Flagstaff, Arizona in 1986. It...
Read More
Bench Trick Guiding Principles
What is a bench trick? A shortcut? A faster way of doing something? A better method? A tool used for...
Read More
Platinum Finishing 1 – Safety
My finishing techniques are up close and personal. The majority of my polishing work is done at the same proximity...
Read More
Tips on Learning Website Basics
In today's internet driven market place you need to have a website whether you are a small "Mom & Pop"...
Read More
How to Handle the Flexshaft
In the course of my 30 years in the jewelry industry, I can recall many instances of damaged equipment and...
Read More
MJSA Custom Jeweler – Brenda Smith
An Uncustomary Request - Creative freedom and some unusual pearls helped create an award-winning necklace by Brenda Smith.
Let’s say...
Read More
2017 Pantone’s Top 10 Colors for Fall
Pantone’s picks are comforting, enveloping, and easy to wear. Warm. Comforting. Effortless. These are just a few of the words...
Read More
Bench Mag Favorite Tips 2002
This article page is from a section "Favorite Tips" from BENCH Magazine 2002 submitted by readers and BENCH Magazine Staff...
Read More
Jewelers’ Stories About Working with Findings
When a commercial finding isn't quite right but making the component by hand seems like reinventing the wheel, creative modification...
Read More
Beyond the Bench: Contemporary Studio Jewelry
Contemporary Studio Jewelry
There are few faster ways to clear a room than to invite a conversation about the difference...
Read More
Slicing Wax Slabs
A drill press (either a full size, miniature, or Foredom) with an end mill or cylinder bur can thin down...
Read More
Reconditioning Beading Tools & Dot Punches
Beading tools and dot punches lose their form and become dull as you use them. You can recondition a tool...
Read More
How to Use the Conduction Soldering Technique
The soldering process, used extensively in all aspects of jewelry manufacturing and repair, joins two or more pieces of metal...
Read More
Customized Beading Tool Retipper, Trays & Polisher
Steve Satow shares his procedure on how to customize bench tools like a beading tool retipper, small parts trays and ...
Read More
3 Tips to Overcome Workplace Dysfunction
My kids are grown now, but I still recall how effective they were at pushing each other’s buttons when they...
Read More
How to Make Straight Wire Holders
Stuller had the foresight to offer straight wire that we don't have to remove the bend from before we use...
Read More
Customized Solder Holder, Jet Sett, Blast Shield
Steve Satow shares his procedure for customized solder holder and blast shield, and how to make using a Jet Sett...
Read More
Safety Issues and Litigation
After writing my recent safety book something unexpected happened. I had a number of calls from lawyers about safety issues....
Read More
Metalsmith ’85 Summer: Health Hazards Q&A’s
This article page is from a segment of the Metalsmith Magazine (1985 Summer), “Health Hazards”, discussing questions from readers and...
Read More
Cutting Down Repair Costs
Much of my business comes from re-cutting colored gems that have been chipped, scratched and broken (not always by the...
Read More
Patination Sources from the Internet
Here are some patination sources on the internet.
Remember that all patinas are toxic and irritant and should not...
Read More
Bench Mag Favorite Tips 2002 Part 4
This article page is from a section "Favorite Tips" from BENCH Magazine 2002 submitted by readers and BENCH Magazine Staff...
Read More
Customized Turntable Tool Rack
Find a turntable that
is size appropriate for
your bench. In this case
mine is 18 inches wide.
If possible...
Read More
Trade Show Marketing Tip
At most trade shows, you could stock up on enough pens, notepads, tote bags, and keychains to start a thriving...
Read More
How Jewelers Approach Work Materials
This diagram shows how jewelers approach working in the field in terms of how they relate to the material. The...
Read More
Metalsmith ’83 Fall: Health Hazards Q&A’s
This article page is from a segment of the Metalsmith Magazine (1983 Fall), "Health Hazards", discussing questions from readers and...
Read More
How to Construct a Portable Photographic Studio
The successful documentation of finished work is of vital concern to every artist. Excellent slides make better teaching tools, and...
Read More
Tool and Equipment Checkpoints
Maybe you’re shopping for the latest technologies—the newest developments in CAD/CAM to produce life-like renderings, a laser to engrave your...
Read More
How to Modify Wooden Ring Clamps
One persistent daily challenge a bench jeweler faces is trying to figure out the best way to hold onto tiny,...
Read More
Buffer System & Ultrasonic Basket Replacement
Buffer System & Ultrasonic Basket Replacement
When we replaced our vacuum tubes for the buffer system I chose to run...
Read More
Bench Mag Favorite Tips 2002 Part 3
This article page is from a section "Favorite Tips" from BENCH Magazine 2002 submitted by readers and BENCH Magazine Staff...
Read More
Bench Mag Favorite Tips 2002 Part 2
This article page is from a section "Favorite Tips" from BENCH Magazine 2002 submitted by readers and BENCH Magazine Staff...
Read More
2 Tips for a Successful Jewelry Collection
In times of increased price competition and global producers, cooperation with designers is also an important factor for large jewelry...
Read More
Metalsmith ’84 Summer: Health Hazards Q&A’s
This article page is from a segment of the Metalsmith Magazine (1984 Summer), “Health Hazards”, discussing questions from readers about ...
Read More
Metalsmith ’84 Spring: Health Hazards Q&A’s
This article page is from a segment of the Metalsmith Magazine (1984 Spring), “Health Hazards”, discussing questions from readers about...
Read More
5 Holiday Casting Process Tips
The hazy days of summer aren’t too soon to begin thinking of designs for the holidays—and how to best cast...
Read More
How to Use Time Fully
Always try to understand, that you are your own best enemy. Be nice to yourself when tackling the unknown. Realize...
Read More
Risking Failure to Master New Things
My grandson has spent the last several weeks learning how to walk. This new risk comes with a lot of...
Read More
How to Make Equally Sized Beads
In this project, I will demonstrate a clever method of making equally sized beads. These beads can be used for...
Read More
Green Bench Tips – Part 1
This is the first in a two-part series on green bench tips shared by jewelers who are taking an eco-friendlier...
Read More
Creating a Whip Burnisher
A worn-out bristle brush can easily be recycled into a useful tool called a whip burnisher or rotary hammer to...
Read More
Bench Mag Favorite Tips 2002 Part 1
This article page is from a section "Favorite Tips" from BENCH Magazine 2002 submitted by readers and BENCH Magazine Staff....
Read More
Bench Jewelers Can Take Sniper Lessons
As the target comes into focus and the operator aligns the crosshairs, elements of the world slowly cease to exist...
Read More
Book Review – Jewelry Contemporary Design and Techniques
Today's metalsmith and jewelry designer has available a full range of reference books—from the general text, which gives a broad...
Read More
From The Bench: Kohler Company
Kohler Company
During April and May of 1993 I was a resident artist at the Kohler Company factory in Sheboygan,...
Read More
Creative Imagination – Undeveloped Resource
In 1959, Victor Papanek gave the third-year students in his creative engineering seminar at Ontario College of Art this problem:...
Read More
The Art of Self Promotion
The art of self-promotion is less about celebrity than it is about perseverance. Breaking into print doesn't take a magic...
Read More
Green Bench Tips – Part 2
This is the second in a two-part series on green bench tips shared by jewelers who are taking another approach...
Read More
4 Marketing Tips for Mobile Customers
Since the advent of the Information Age, the marketing landscape has undergone a radical transformation. Pre-internet, businesses used to be...
Read More
Discover New Customers
Consumers still want to buy and wear jewelry. You’re just going to have to leap to reach them. Confront the...
Read More
Art and Technics: Learning from History
This article is one of a series of articles from Metalsmith Magazine “Art and Technics” talking about techniques in craftsmanship...
Read More
Metalsmith ’83 Summer: Health Hazards Q&A’s
This article page is from a segment of the Metalsmith Magazine (1983 Summer), "Health Hazards", discussing questions from readers and...
Read More
How to Customize Curved Tip Melee Tweezers
These tweezers are great for gripping melee when straight tips don't give you enough clearance. They allow you to slide...
Read More
Metalsmith ’84 Fall: Health Hazards Q&A’s
Linda Weiss-Edwards provides a list of Onsite Consultation for Artists and Schools from each state in the United States in...
Read More
The Prospective General Teacher of Art
The teacher of vocational courses in art should be thoroughly trained in his craft and, if possible, should be a...
Read More
From the Bench: Sisyphus
From the Bench: Sisyphus
In the city where I grew up – Chicago – the ghettos were literally crumbling. My...
Read More
Recent Sightings: Jewelry Teachers
This article series from Metalsmith Magazine is named “Recent Sightings” and here Bruce Metcalf talks about art, craftmanship, design, the...
Read More
Recent Sightings: Handwork
This article series from Metalsmith Magazine is named “Recent Sightings” where Bruce Metcalf talks about art, craftmanship, design, the artists,...
Read More
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.