Contributions From George W. Fischer
Gemstone Coloration and Dyeing – Introduction
The prime requisite for coloration of gemstone is that it be porous . That is to say there must be...
Read More
Gemstone Coloration and Dyeing – Iron Process
There are several reactions well known to chemists, involving iron compounds and prussiate compounds (ferrocyanides and ferricyanides) that yield characteristic...
Read More
Gemstone Coloration and Dyeing – Cobalt Series
The use of cobalt compounds to impart blue hues to glass, glazes and enamels has been known for centuries. "Cobalt...
Read More
Gemstone Coloration and Dyeing – Copper Series
Various and attractive shades of blue can be induced in gemstone by the use of copper compounds. This is perfectly...
Read More
Gemstone Chemical Coloration Techniques
The most important detail in the preparation of gemstone for chemical coloration is that it be clean. Oil and grease,...
Read More
Gemstone Coloration and Dyeing – The Blacks
There are only two ways that I know of to induce black into gemstone. One of these involves carbon while...
Read More
Gemstone Coloration and Dyeing – Pinks and Reds
There are only a few inorganic processes, in my experience at least, that will impart pinks or reds to gemstone....
Read More
Gemstone Coloration and Dyeing – Browns and Yellows
At first consideration, it might seem poor organization to include browns and yellows in the same chapter. However, I do...
Read More
Gemstone Coloration and Dyeing – The Greens
It seems that everyone likes the greens in chemically colored gemstone. Probably this is because greens are almost universally pleasing...
Read More
Gemstone Coloration and Dyeing – Table of Contents
This book is the culmination of some twenty-five years of personally supported research on the use of inorganic chemicals to...
Read More
Chemically Induced Inclusions – Copper Inclusions
Since the discovery that the principle of electrochemical displacement of metals can be used effectively and easily to induce inclusions...
Read More
Chemically Induced Inclusions – Dendrites Moss Plume
Dendrites, moss, plume and similar inclusions have added interest
and value to gemstone for about as long as man has...
Read More
Chemically Induced Inclusions – Tin Inclusions
Tin inclusions can be induced in agate and other gemstone varieties in much the same way as with copper. Just...
Read More