Contributions From Arthur Anton Skuratowicz and Julie Nash
Working with Topaz
The primary issue with topaz that must be remembered at the bench is its one perfect cleavage direction. Hammering or...
Read More
Working with Pearls
Both natural and cultured pearls are formed when an irritant lodges in a mollusk. The mollusk then deposits layers of...
Read More
Tanzanite Gemstones
Due to tanzanite fragile nature, the stone is very easy to abrade, scratch, or chip during the setting process. When...
Read More