Lapis Lazuli Gemstone Properties


Lapis lazuli differs from other gem materials because it is a "rock" composed of several minerals rather than being a single mineral as the other gemstones are. The components of lapis lazuli include sodalite minerals, calcite, and pyrite. The sodalite minerals are the blue part, the calcite is white, and the pyrite is the "gold flecks" commonly visible in lapis lazuli. The finest quality is a dark, but still intense blue color with no visible calcite and a mere sprinkling of pyrite. "Royal blue" is a descriptive term for fine material. All lapis lazuli is opaque. If there is quite a bit of calcite the material is a lighter blue; this can still be nice as long as there are no visible portions of calcite. As the color becomes lighter the value of lapis lazuli drops, visible calcite is a definite detriment. Quality of cutting is a value consideration also.

2 Minute Read

HomeLearning CenterLapis Lazuli Gemstone Properties
By Sondra FrancisMore from this author

Lapis lazuli differs from other gem materials because it is a "rock" composed of several minerals rather than being a single mineral as the other gemstones are. The components of lapis lazuli include sodalite minerals, calcite, and pyrite.

The sodalite minerals are the blue part, the calcite is white, and the pyrite is the "gold flecks" commonly visible in lapis lazuli. The finest quality is a dark, but still intense blue color with no visible calcite and a mere sprinkling of pyrite. "Royal blue" is a descriptive term for fine material.

All lapis lazuli is opaque. If there is quite a bit of calcite the material is a lighter blue; this can still be nice as long as there are no visible portions of calcite. As the color becomes lighter the value of lapis lazuli drops, visible calcite is a definite detriment. Quality of cutting is a value consideration also.

Lapis Lazuli
(Photo by ICA/Bart Curren)

Lapis Lazuli Gemstone Properties

Colors:Shades of blue
R.I.:1.50
Durability:Fairly tough
S.G.:2.70 - 2.90
Treatment:Dyeing is common
Hardness:5 - 6
Availability:Supply meets demand
Localities:Afghanistan and Chile
Price:Low to moderate
Common shapes:Cabochons of all shapes, beads and carvings

The finest qualities of lapis lazuli are mined in Afghanistan from a mine that has been in operation for 7,000 years! Chilean lapis lazuli generally contains large amounts of calcite.

Very inferior qualities of lapis lazuli are dyed. You can detect this by rubbing a cotton swab soaked in acetone (or fingernail polish remover) across the surface of the stone; be patient, it may take a minute or two. If blue coloring comes off and stains the cotton the material is definitely dyed.

Generally dyed material should be avoided; dyed beads can bleed onto clothing or skin if the material gets wet. Earrings and rings can fade or loose their color especially if they come in contact with strong chemicals. Be sure you know whether the material is dyed or not when you buy it. Have the seller write "natural" or "dyed" on the sales slip.

If the items is really cheap and you know it's dyed and are aware of the potential problems then buy it. Otherwise, ask intelligent questions about lapis lazuli and ask that the seller test for you or test it yourself. This can be a lot of fun!

See also:
By Sondra Francis – Copyright © Sondra Francis, G.G. 1999
_____________________________
About the Author
Sondra Francis has scoured every major colored gemstone market in the world since 1978. She was a charter member of the American Gemstone Association and served as a board member. She was a founding member of the International Colored Gemstone Association. A true gem lover, Sondra has marketed her treasures on the wholesale and retail markets.
_____________________________
Acknowledgments: A special thanks to Pam Dulgar, Alex Edwards, Cheryl Kremkow, Kate Kirby, Helen Mitchell, Carol Morgan Page, David Pond, Elaine Proffitt, and Ray Zajicek for their help.
Photographs: Bart Curren and ICA Gembureau ; Alex Edwards, Pearl Sales Institute ; David Dikinis

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Sondra Francis

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.