Working with Jewelry Hinges Made Easy
Sometimes working with jewelry hinges can be too taxing. And not knowing how will make your work even harder. Here's a how-to on working with jewelry hinges.
1 Minute Read
Sometimes working with jewelry hinges can be too taxing. And not knowing how will make your work even harder. Here's a how-to on working with jewelry hinges.
Ball Based Hinges
On small plastic boxes, are sometimes found, hinges that snap into place to allow easy assembly. They are made with two balls attached to the lid and a disc with dimples in each side attached to the bottom of the box. The lid snaps on and then can swivel as the balls slide in the indentations in the disc.
While metal does not have the flexibility that plastic does. A version of this hinge can be built where the spheres are pinched slightly together after inserting the indented disc. Such a hinge can come apart if pulled on hard enough but will function well if there is little stress on it.
One can reverse the positions of the rounded parts by having the central 'knuckle' have rounded ends and be installed in sturdy tabs with rounded indentations on the other side of the hinge. It is designed so that they are open enough to just squeeze in the middle 'knuckle' and then are closed over its rounded ends to install the hinge.
Strip Hinges
Alternative hinges (coils, sewing, fiber, fabric, mesh, chains)
Related Linkages
Since we defined a hinge as involving rotation of parts relative to each other at a fixed point somewhere back in the beginning there are a number of other kinds of solutions which satisfy this definition. Examples of this include coil bindings on notebooks, sewing through holes in the material, glued or mechanically fixed cloth or woven materials, mesh use and all sorts of chains and jump ring based flexible systems.
Solving Design Problems
Example of hinge with bezels on end-use as thinking example-spell out analysis steps
An example of how this kind of thinking is applied can be seen in this design sent to me by Phil Porier. He has used a hinge pin just shorter than the hinge itself on each side and then tube set faceted round gems into the ends of the hinge. I might recommend starting with the outer knuckles a little wider than the width being hinged: this to allow for metal removal during setting.
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.