Simple Method of Forming Jump Rings


This paper describes a simple process of forming jump rings. These jump rings were formed from 16 guage sterling silver wire. The links will be 1/2 inches in diameter and will be used to create a pottery shard link concho belt..

1 Minute Read

HomeLearning CenterSimple Method of Forming Jump Rings
By Lee EppersonMore from this author
Updated on

This paper describes a simple process of forming jump rings.

These jump rings were formed from 16 guage sterling silver wire. The links will be 1/2 inches in diameter.
The links will be used to create a pottery shard link concho belt.
A groove is cut into the end of a ½ inch round wood dowel. The groove will be used to hold the wire at the beginning of the wire wrapping process.
The end of the wire is bent at a 90-degree angle and placed in the groove of the dowel as shown.
The wire is wrapped around the dowel. Wrap the wire around the dowel until there will be enough links for the project.
The wrapped loops are slid off the dowel and placed on its opposite end. Saw cut a groove through the center of the dowel as shown. The wire links are moved against the saw blade as they are cut off.
The links will fall onto the saw blade as they are cut free from the main body of links.
This is what the links will look like.
Loops are soldered on opposite sides of the pottery shard. The link is then passed through the loop on two shards. The link is then closed and soldered.
By Lee Epperson – © 2005
All rights reserved internationally. Copyright © Lee Epperson. Users have permission to download the information and share it as long as no money is made. No commercial use of this information is allowed without permission in writing from Lee Epperson

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Lee Epperson

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.