The New MJSA/WGC White Gold Color Index
Have you ever noticed how white gold varies in color? Many folks think white gold is the same color as rhodium because all the white gold they ever saw was plated with rhodium. Others who have bought very inexpensive white gold have seen the "real" color and all too soon due to a very thin plating job. That can be frustrating. Most of us are aware that the white color comes from the alloy used. Manufacturers are very aware of the consequences of the different white alloys. Some of us are allergic to nickel in contact with the skin. In Europe a restriction was imposed in response to the allergy suffered by some people. Even jewelry that complies with the restriction can cause allergic symptoms. As a result non nickel white gold is often the choice there. If you increase your understanding you will make better white gold...
4 Minute Read
Have you ever noticed how white gold varies in color? Many folks think white gold is the same color as rhodium because all the white gold they ever saw was plated with rhodium. Others who have bought very inexpensive white gold have seen the "real" color and all too soon due to a very thin plating job. That can be frustrating.
To address this and other issues Kraftwerks, MJSA, and the WGC all worked together to form the White Gold Task Force. Kraftwerks had the easy role, we just held a white gold roundtable to discuss the issues. As it so happens at Kraftwerks we had Jim Marquart from MJSA and Chris Corti from the World Gold Council sitting in. Between those guys and a few key operators and users of white gold we started something important at that discussion. MJSA and WGC did the hard parts.
Most of us are aware that the white color comes from the alloy used. Manufacturers are very aware of the consequences of the different white alloys. Some of us are allergic to nickel in contact with the skin. In Europe a restriction was imposed in response to the allergy suffered by some people. Even jewelry that complies with the restriction can cause allergic symptoms. As a result non nickel white gold is often the choice there. If you increase your understanding you will make better white gold. You will save money too.
In the United States we use nickel 95% or more of the time to make white gold. The rest of the time we use palladium. Anytime we use more nickel the jewelry is harder to produce. When we use high amounts of palladium the jewelry becomes more expensive. A few rare exceptions exist including at least one patented manganese white gold from Precious Metals West.
When we reduce the amount of whitener (nickel or palladium) to reduce the temperatures needed for casting, or the expense, or to make a more malleable nickel white gold the color is compromised. As it turns out the key factor to the consumer is the degree of yellowness present in the finished item. A tint of gray or green is less objectionable to most consumers than yellow. This is due to the yellowness of gold and the way the eye works. Shame on the cheater who rhodium plates over yellow!
To accurately measure the color of white gold the WGTF turned to GretagMunsell. This is a company that does color science and makes color samples for all kinds of industries. Paint, ink, paper and now white gold all can be measured by a color spectrophotometer. The chosen color technology is the ASTM YID1925. The "yellowness index". The higher the number the more yellowness is visible in the sample.
To be called white gold the yellowness must be less than 32. It would be deceptive to call any gold with a YID at 32 or higher "white gold". Call it beige or crème or tan but not white.
The best white gold color does not require rhodium. This is what we call grade one white gold. Sometimes the term premium white is used but we prefer not to use that term for mere color. Perhaps more expensive high palladium content whites deserve that term. Yellowness or YID less than 19. For comparison, platinum comes in with a YID of 9.5 and pure silver is in the YID 7 range.
The next grade of white "grade two white gold" has a tone that makes rhodium optional. Lots of jewelry is made with white gold that is this color. This is the range from a YID of 19 to 24.4.
The lowest grade of white gold is grade three. YID from 24.5 to 32. This color requires rhodium plating. Good long lasting plating. This white has a distinct but slight yellowish tone.
Understand that there was some compelling reason to use this grade three range of alloys. Expense, or malleability and setting considerations reduced the whitener to the lowest acceptable amount. Try anticlastic raising sometime with grade one nickel white and see what you get. Most likely cracks in the gold and shattered confidence in the designer!
You can get equipment to find out what grade your white gold is. MJSA distributes the Color index card with accurate foil samples on a black background and the calibrated light sources. Use the foil sample chart in a calibrated light box or under the right desk lamp light source to compare your gold with the index. If you have any eye for color at all you will quickly see what category your white gold falls into. For the GG this is grade school work. If you need to know exactly what the yellowness index is for your gold you must send it in to a company that has a Spectrophotometer from Munsell. MJSA can refer you to these firms.
These standards are voluntary and flexible. If the WGTF is found to have been too generous or too strict the numbers may shift a small amount. Every effort was made to include people from retail, manufacturing, alloy manufacturing and metallurgy. They were put on the panel to balance the interests. We sampled dozens of white golds to find the right range of color. For more information contact MJSA and ask about the white gold index.
Read also: Going the White Way - Working with White Gold
The award-winning Journal is published monthly by MJSA, the trade association for professional jewelry makers, designers, and related suppliers. It offers design ideas, fabrication and production techniques, bench tips, business and marketing insights, and trend and technology updates—the information crucial for business success. “More than other publications, MJSA Journal is oriented toward people like me: those trying to earn a living by designing and making jewelry,” says Jim Binnion of James Binnion Metal Arts.
Click here to read our latest articles
Click here to get a FREE four-month trial subscription.