Making Silver Whistles


Okay, so this is a bit esoteric. I mean, how many people do you know that make silver whistles. It all started with a commission from a captain of a racing yacht. He had lost his whistle and he wanted me to make one that also had the shape of a Christian Cross. He uses it to whistle to his crew when they racing, because the wind and sea drown out his voice. (no pun).

4 Minute Read

HomeLearning CenterMaking Silver Whistles
By Hans MeevisMore from this author
Updated on

Okay, so this is a bit esoteric. I mean, how many people do you know that make silver whistles. It all started with a commission from a captain of a racing yacht. He had lost his whistle and he wanted me to make one that also had the shape of a Christian Cross. He uses it to whistle to his crew when they racing, because the wind and sea drown out his voice. (no pun)

This was the captains whistle.
%image_alt%
This is the whistle that will be made in this Hidi.

So a year or so goes by, and one day I wake up and I realize  that I can't actually remember, how I had made the captains whistle. Luckily I had, in my research, made four or five test samples, firstly out of copper tubing and then out of silver, and I still had these attempts in my silver junk box. So I decided to make this Hidi , quickly, before I forget even more! I am sure that my loss of memory is to do with the fact that my eyebrows and hairline are at war…..

imgWe start with a piece of flat, annealed silver, the size shown. I rolled this down to 0.8mm thick, but I am sure other thicknesses will be good too, like 1mm or 1.2mm.
imgI bend it round and solder it up into a tube that has a diameter of 11mm on the inside.
imgThen I saw it about a third of the way up. The first picture shows the whistle to be 60mm long. In actual fact it turned out to be 50mm long. The reason is that the longer the front of the whistle is the lower the pitch. And the shorter, the higher the pitch. I decided on the pitch by suddenly and unexpectedly blowing the whistle behind my wife, and then seeing how high she jumped. I settled in a six inch jump which made the whistle 50mm. ( semi kidding 🙂
imgThe front section of the whistle is cut out as shown. The depth of the cut is 5.5mm. The thickness of the 'posts' is 5mm. Those measurement are not finite. There is, within reason  quite a variable.
imgNow comes the critical part. This plate is .5mm thick. I pierce it out carefully.
imgThen I file the lips just so that the plate fits very snugly into the bottom section.
imgThen I solder in the plate so that it is a millimeter or so recessed from the top. Also, I have run a .7mm barrel bur so that the plate and the inner walls have an equal gap. This is all rough still. I will take sandpaper strips and smooth the .7mm gap out and  use bristle brushes and brush finish the inside later.
imgAt this stage I can hold the two pieces together and make the thing whistle. It's a bit finicky, but at least I know it will work.
imgNow I need to make the mouth piece. I roughly shape a 'washer' of silver.
imgWhich is filed to about the same diameter as the whistle section. It is about 9mm wide, but in retrospect I could have made it 11mm wide. It would fit my teeth and lips better when blowing the whistle.
imgThen I file it with a 6mm rattail file (a round file that is not tapered) and make a circle of  silver. The wire is 2mm thick.
imgThis circle I solder on just so that the bottom part of the whistle will fit in snugly. This looks good and hides the joint.
imgThen I make a flat washer 2mm thick and solder that onto the other side of the mouth piece.
imgLike this.
imgHere I am about to solder the two components together.
imgThese are the three sections of the body of the whistle.
imgThe bottom piece soldered to the mouth piece.
imgThen Hans decided to become clever. This is always dangerous. So instead of just putting a nice gold cap on the end of the whistle, why not put a amethyst there instead. Bad idea. The whistle simply ceased to whistle. I assume the pavilion of the stone upset the air flow. If I were to solder at the top tube closed and then mount the stone on top of that, it would work. But I was too far advanced to start messing around with something that was certain to end in tears so…
imgI soldered a gold cap on instead.. The two grooves are there to accept the bail of the whistle
imgWhen the whistle is soldered together, it is essential that the posts and the whistle plate align. The whistle will not work if they are at 90 degrees to the posts.
imgHere the whistle is soldered together, ready to be finished off.
imgAnother view.
imgFinished off.
By Hans Meevis – © 2008
All rights reserved internationally. Copyright © Hans Meevis. Users have permission to download the information and share it as long as no money is made. No commercial use of this information is allowed without permission in writing from Hans Meevis

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.