Let’s talk Gemstones – Staurolite


Staurolite! Why would one of the most ordinary, patently unattractive minerals, used as a religious talisman and a good luck charm for centuries, be, in its transparent faceted form, a much sought after collector's gem? Rarity! Seldom do the dark reddish-brown or yellowish-brown transparent crystals occur in sufficiently light tones and sizes to warrant faceting.

4 Minute Read

HomeLearning CenterLet’s talk Gemstones – Staurolite
By Edna B. AnthonyMore from this author
Updated on

Staurolite! Why would one of the most ordinary, patently unattractive minerals, used as a religious talisman and a good luck charm for centuries, be, in its transparent faceted form, a much sought after collector's gem? Rarity! Seldom do the dark reddish-brown or yellowish-brown transparent crystals occur in sufficiently light tones and sizes to warrant faceting. Its fair dispersion of 0.023 is usually masked by its excessively dark tones. A sparkling two-carat staurolite gem would certainly be a true prize.

Idiochromatic staurolite develops in regional metamorphic rock formations. In petrology, it is used as an index mineral to define the grade and type of the host rock. Staurolite rarely occurs in massive form. It occurs more often in opaque, interpenetrant, twinned forms at sixty degree, as in St. Andrew's cross, or ninety degree, as the Greek cross, orientations than in individual prismatic crystals. The cruciform shape gives it its name derived from the Greek words stauros (cross) and lithos (stone). Layers of chains of AlO8 octahedra parallel to the C axis alternate with layers of Fe2AlO3(OH) in its nesosilicate structure. There is normally the replacement of some of the Fe2+ by magnesium, with Fe3+ replacing a portion of the aluminum. Dr. Frederick H. Pough states in his A Field Guide to Rocks and Minerals that "it can be regarded chemically as a mixture of kyanite and iron hydroxide." Although it is slightly affected by sulfuric acid, the mineral is infusible and virtually insoluble in acids. After firing, it crushes to a slightly magnetic brown powder. The streak of fresh material is colorless.

Both the Color Encyclopedia of Gemstones by Dr. Joel Arem and the Manual of Mineralogy list its crystal system as monoclinic (pseudo-orthorhombic), but other sources classify it as orthorhombic. A distinct plane of cleavage exists, and the fracture of this brittle substance is conchoidal to uneven. A density range from 3.65 to 3.83 with a hardness of 7 - 7.5 is typical. The lustre and fracture lustre can vary from vitreous to resinous to dull, and a pocked surface may appear if a degree of alteration has occurred. Its normal refractive indices [a=1.739-1.747; b=1.745-1.753; y=1.752-1.761] increase with the iron content. The birefringence of this biaxial positive mineral has a range of 0.011 to 0.015. Golden yellow/red or yellow/colorless are its distinct pleochroism colors. A strong band at 4490 and a weak one at 5780 occur in the non-diagnostic spectrum. Exposure to long-wave and short-wave ultraviolet light causes no reaction.

With the presence of a trace of zinc, lighter colors occur in zincian staurolite, and some of its optical and physical properties differ slightly. A specific gravity of 3.79 is normal. Its refractive indices range from 1.721 - 1.731. Beyond 4900, the spectrum is absorbed, but weak narrow bands occur at 5315 with wide strong bands exhibited at 6100 and 6320. Yellow/green/red are its trichroic pleochroism colors. Zincian staurolite might even be considered a color-change gem since it may appear yellow-green in daylight and red-brown in incandescent light. Generally, it is from this material from Switzerland or Brazil that the rare gemstones are cut.

Rock-forming deposits of strongly pleochroic lusakite, a deep blue opaque staurolite, where cobalt and magnesium replace iron, are located in Lusaka, Zambia. The lusakite is extracted from the formations and used as a pigment.

Staurolite has been known by many names. Mineralogists and geologists will be familiar with staurotide and grenatite. Fairy stones, fairy crosses, and cross stones are abundant in North Carolina, Virginia, Georgia, and Tennessee. They are worn as amulets and good luck charms. Imitations are carved from fine grained clay rock and dyed. A source near Taos, New Mexico produces fine twinned staurolite. Deposits in Connecticut, Maine, Vermont, New Hampshire, Canada, Scotland, France, some alluvials in the Urals and the Gorob mine in Namibia are other sources. Staurolite found in Sweden contains a significant amount of manganese. Kyanite accompanies the twinned staurolite recovered from the mica-schists of Monte Campione and Lake Ritone in Switzerland. Names used here are Lapis crucifix and Baseler Taufstein (Basle baptismal stone). Columnar crystals of staurolite also occur with kyanite in these white schists and are striking mineral specimens.

Collectors of mineral specimens usually have staurolite specimens in their cabinets. However, a fair-sized clean light-colored faceted staurolite gem is a real treasure that few possess.

Staurolite Gemstone Properties

Speciestaurolite
Composition:[FeMg]2[AlFe]9 O6 [SiO4)4 [O,OH]2+Zn or +Co Hydrous iron-aluminum silicate
Class:silicate
GroupA2 SiO5
Species:staurolite
Crystal System:monoclinic; pseudo-orthorhombic; orthorhombic
Variety:staurolite; zincian staurolite
Colors:dark brown, reddish brown, dark blue, and black
Phenomena:color-change? see narrative
Streak:colorless or light gray
Diaphaneity:opaque, translucent, and rarely transparent
Habit:columnar, prismatic, typically twinned, and rarely massive
Cleavage:distinct in one plane
Fracture:conchoidal to uneven
Fracture Lustre:resinous
Lustre:vitreous to resinous to dull to earthy
Specific Gravity3.65 to 3.83
Hardness7 to 7.5
Toughness:fair
Refractive Index1.721 to 1.761; see narrative
Birefringence:0.011 to 0.01
Optic Characterbiaxial positive
Dispersion:0.02
Pleochroismdistinct trichroic; less red or yellow/golden yellow; zincian staurolite: yellow, green, red
Luminescenceinert
Absorption Spectrumsee narrative
Aqua Filterno information
Chelsea Filterno information
Solubilityaffected slightly by sulfuric acid; virtually insoluble in acids
Thermal Traitsinfusible
Treatmentsoiling of cross stones
Inclusionsno information
Related Links:

Let's Talk Gemstones - Opal Part 1
Let's Talk Gemstones - Opal Part 2
Let's Talk Gemstones - Peridot
Let's Talk Gemstones - Zircon Group

By Edna B. Anthony, Gemologist
All rights reserved internationally. Copyright the New Mexico Faceters Guild © 2002 Users have permission to download this information and share it as long as no money is made. No commercial use of this information is allowed without written permission from the New Mexico Faceters Guild
____________________________
The purpose of the New Mexico Faceters Guild (NMFG) is to bring together persons who are interested in faceting or faceted stones. We promote the art and science of faceting and provide a means of education and improvement in faceting skills. Finally, we provide a means of communication between those persons involved or interested in faceting as a hobby.
____________________________
Meeting Dates: Second Thursday of odd numbered months
Time:   7:00 PM
Place: New Mexico Museum of Natural History
    1801 Mountain Road NW
    Albuquerque, NM USA

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Edna B. Anthony

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.