Installing New Tapered Bezels
This ring is in for repair and reconstruction. When it was originally made, 6-prong settings were used to mount the customers diamonds. All prong tops are severely worn and one prong has broken. The customer has requested bezel settings, so the prong settings were removed from the ring. The ring was re-sized according to the customers request and then pre-finished. For tacking the tapered 14-karat yellow gold bezels, the brass tweezers lead was modified to firmly hold a bezel. A ball bur was used to remove metal from inside each end of the tweezers.
1 Minute Read
This ring is in for repair and reconstruction. When it was originally made, 6-prong settings were used to mount the customers diamonds. All prong tops are severely worn and one prong has broken (arrow).
Important
Tack-, fusion- and pulse-arc equipment settings will differ and are based upon the volume, amount of contact and alloy of the material you are working with. Practicing using like materials will give you a parameter for the settings required for your application. Keep a record of settings and tasks for future reference.
You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.
The All-In-One Jewelry Making Solution At Your Fingertips
When you join the Ganoksin community, you get the tools you need to take your work to the next level.
Trusted Jewelry Making Information & Techniques
Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.