Steve Satow shows the procedure for a customized earring setting pliers using a normal setting pliers.

Normal setting pliers can be modified to set stones in loose heads and earrings.

Please wear your safety glasses. Most setting pliers have a groove in the top. Take a pair of separating disks stacked on one flex shaft mandrel and start to grind a groove through the top of the pliers where they are already grooved.

Continue the cut all the way to the back as shown in this picture. Make sure the groove is wide enough for an earring post to fit through.

Now cut a sideways notch at about a 45 degree angle as pictured. This is where the base of the head rests; keeping it tight while you bend over the prongs.

This is a profile shot of the pliers in action. It works well on 3, 4, 6 and 8 prong heads.

By Steve Satow
© Bench Magazine – 2006 Fall
In association with
BENCH Magazine is devoted to the Bench Jeweler in retail jewelry stores and small trade shops.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.