How to Customize Fine Tip Melee Tweezers


These tweezers are great for gripping melee when you slide then into position in continuous channel setting jobs. Here you see the very fine tips on these tweezers.

0
HomeLearning CenterHow to Customize Fine Tip Melee Tweezers
By Steve SatowMore from this author
Updated on

This article by Steve Satow shows how to customize fine tip melee tweezers for channel setting using melee tweezers # 115-005.

How to Customize Fine Tip Melee Tweezers

These tweezers are great for gripping melee when you slide then into position in continuous channel setting jobs. Here you see the very fine tips on these tweezers.

Customize Fine Tip Melee Tweezers

Measure down the tips until they are 0.5 mm wide and make a mark.
Please wear your safety glasses for all the grinding on this project. use a separating disc to cut the tips off evenly where they are marked.
Use your separating disc to grind a 45 degree angle on both tips.
Use a diamond wheel to dress the edge of your separating discs until it comes to a sharp edge. Make sure the sharp edge is even on both sides.
With your sharpened disc score a groove about 0.25 to 0.5 mm from each end.
Try to hold a melee and if necessary make your grooves on the tips deeper until you can hold melee securely.
Close up of the tips with the grooves cut in them. These tweezers make it a lot easier to handle melee with out them flying.
By Steve Satow – © 2012
All rights reserved internationally. Copyright © Steve Satow. Users have permission to download the information and share it as long as no money is made. No commercial use of this information is allowed without permission in writing from Steve Satow.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.