Channel Setting Bezels with Customized Pulling Pliers


These pliers are used to pull back bezels on channel set rings. This allows you to drop in the stones without thinning the edge to allow the stone to drop in. It works especially well with the continuous channel method that the all-set tool creates. Mark the bottom jaws about 0.25 in from the end.

1 Minute Read

HomeLearning CenterChannel Setting Bezels with Customized Pulling Pliers
By Steve SatowMore from this author
Updated on

This article by Steve Satow shows how to make a customized pulling pliers for channel setting bezels using pulling pliers #111-137.

Customizing your pulling pliers

These pliers are used to pull back bezels on channel set rings. This allows you to drop in the stones without thinning the edge to allow the stone to drop in.

It works especially well  with the continuous channel  method that  the all-set tool creates. Mark the bottom jaws about 0.25 in from the end.

Use a separating disc to cut off the tip.
Use a abrasive wheel to make a gently rounded end on the bottom jaw.
Mark the upper jaw where the lower jaw ends. Open the jaws in order to heat them.
Heat the tip until cherry red. Then close the jaws and pound the tip of the upper jaw around the tip of the lower jaw.
Round the tip until the end has a gentle curve both around the end and on the inside of the tip. The curve on the inside allows you to pull metal without tearing  at the outside corners.
Test the tips to make sure they will grip the bezel correctly.
Open your dividers to the depth you would normally set the stones. Scribe a line inside the channel on both sides.

Cut a groove with a allset tool or if your steady enough freehand.

Cut a piece of silver solder to use as a scratch shield.
Place the piece of solder between the jewelry and the pliers.
Gently pull back on the bezel move to the side and pull a little more until you can easily slide in one of the stones your setting.
You can see how the metal pulls back easily.

After you have all the stones in place you can use some bee's wax to make them all stay until you tighten the bezel. Then steam away the wax.

Side view of ring with no dent because we used the silver solder as a shield.
%image_alt%Because we pulled back the metal we didn't have to do a deeper undercut on one side to allow the stones to drop in.

This often makes one side of the bezel thinner or makes us use bezels thicker than we need to make sure their heavy when were done polishing. Here we never bur the metal away we just pull it back.

By Steve Satow – © 2012
All rights reserved internationally. Copyright © Steve Satow. Users have permission to download the information and share it as long as no money is made. No commercial use of this information is allowed without permission in writing from Steve Satow.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.