3M XR wheels, formerly known as XK wheels are ideal for sprue removal and smooth deburring with minor surface reduction. A channel can be created in the wheel for repetitive multiple part processing. They replace stone wheels, have superior edge retention and last up to 4 times longer. The side of the wheel can be used as a lap to produce crisp edges and they generate less waste than conventional wheels..

2 Minute Read

HomeLearning Center3M Bur and Polish Wheels
By Mark B. MannMore from this author
Updated on

Below are the 3M XR, Scotch-Brite, Bur an Polish Wheels for you deburring, finishing and polishing needs. Learn more about them.

3M™ XR Wheels

3M™ XR wheels, formerly known as XK wheels are ideal for sprue removal and smooth deburring with minor surface reduction. A channel can be created in the wheel for repetitive multiple part processing. They replace stone wheels, have superior edge retention and last up to 4 times longer. The side of the wheel can be used as a lap to produce crisp edges and they generate less waste than conventional wheels.
Scotch Brite WheelsXR wheels are available in 6 by 1 by 1 1/4 inches and 6 by 1/2 by 1 1/4 inches. They are offered in medium hard and fine hard surfaces. This 6 inch wheel is shown with a 3M™ tapered spindle adapter.
Scotch Brite WheelsI used the XR wheel to remove the sprue and went around the high surface of this 14 karat white gold ring. Sprue removal was quick and generated little wheel waste. Surface reduction was minimal and I created flat even surfaces in less time than hand filing.
Scotch Brite WheelsIn addition to the 6 inch wheels, the XR abrasives are offered in mounted points and used with a flexible shaft at the bench. The shapes are ideal for finer detail.

3M™ Scotch-Brite Wheels

3M™ Scotch-Brite unitized wheels improve precious metal surface finishing without significantly changing the shape or dimension of the workpiece. They are available in a myriad of sizes and shapes and their applications are suited for light deburring, blending and pre-finishing. They run cool, resist loading and help prevent undercutting while providing consistent, uniform finishes as fresh abrasives are continually exposed to the work surface.
Scotch Brite WheelsShown are a general selection of mounted unitized wheels. They are offered in a variety of shapes, grit and sizes. The top row is a kit of permanently mounted points in a variety of shapes available from Stuller. The center row shows Cut and Polish, General Purpose and EXL unitized Scotch-Brite wheels.
Scotch Brite WheelsUsing a unitized bullet cone from the Stuller kit, I was able to remove minor surface irregularities from this 14-karat yellow gold earring casting. The small pointed shape allowed me to access the inner circular area without damaging or gouging the outer surface.
Scotch Brite WheelsHere I'm using a 3A-very fine 3M™ General Purpose Unitized wheel to smooth and even the top surface of this 14-karat yellow gold ring shank. I was able to evenly smooth the rough casting without significant surface reduction.

3M™ Buff and Polish Wheels

Buff and polish wheels are designed to take the place of felt wheels. They hold more compounds, cut faster and last longer. Their sizes range and they can be used with a flexible shaft at the bench or at a polishing machine.
Scotch Brite WheelsBuff and Polish Wheels are made from synthetic fibers and are very durable. This one is 3 by 1 inch and is medium hardness.
Scotch Brite WheelsI'm using the 3M™ Buff and Polish wheel with Foredom's Platinum Blue compound to brighten the top flat surfaces of this 14-karat yellow gold ring.
By€“ Mark B. Mann – Copyright © Mark Mann 2004
Technical Contributions by Andy Kroungold,
Tool and Equipment Expert from Stuller, Lafayette , LA
Photographs by€“ Mark B. Mann
All rights reserved internationally. Copyright © Mark Mann. Users have permission to download the information and share it as long as no money is made. No commercial use of this information is allowed without permission in writing from Mark Mann.

You assume all responsibility and risk for the use of the safety resources available on or through this web page. The International Gem Society LLC does not assume any liability for the materials, information and opinions provided on, or available through, this web page. No advice or information provided by this website shall create any warranty. Reliance on such advice, information or the content of this web page is solely at your own risk, including without limitation any safety guidelines, resources or precautions, or any other information related to safety that may be available on or through this web page. The International Gem Society LLC disclaims any liability for injury, death or damages resulting from the use thereof.


Mark B. Mann

The All-In-One Jewelry Making Solution At Your Fingertips

When you join the Ganoksin community, you get the tools you need to take your work to the next level.

Become a Member

Trusted Jewelry Making Information & Techniques

Sign up to receive the latest articles, techniques, and inspirations with our free newsletter.